AWWA C200 spiral po'lat quvur
video

AWWA C200 spiral po'lat quvur

Spiral po'lat quvurlar asosan suv ta'minoti loyihalarida, neft-kimyo sanoatida, kimyo sanoatida, elektr energetikasida, qishloq xo'jaligini sug'orishda va shahar qurilishida qo'llaniladi.
So'rov yuborish
Hozir chat
Mahsulotni tanishtirish

AWWA C200 SSAW quvur yetkazib beruvchi-GNEE

Spiral po'lat quvur - bu xom ashyo sifatida po'latdan yasalgan po'lat plitadan foydalangan holda avtomatik ikki simli ikki tomonlama suv ostida payvandlash jarayoni bilan payvandlangan spiral tikuvli po'lat quvur, doimiy haroratli ekstruziya kalıplama. Spiral po'lat quvur chiziqni payvandlangan quvur blokiga oziqlantiradi. Bir nechta roliklar bilan o'ralganidan so'ng, chiziq asta-sekin o'ralib, teshik bo'shlig'i bo'lgan dumaloq trubka blankasini hosil qiladi. Payvandlash bo'shlig'ini 1 ~ 3 mm oralig'ida nazorat qilish uchun ekstruziya rolikini kamaytirish miqdorini sozlang va payvandlash bo'g'inining ikkala uchini yuving.

Standart: AWWA C200, AWWA C203, AWWA C205, AWWA C208, AWWA C210, AWWA C213 va boshqalar.

Sertifikat EN10217, EN10219,

Tashqi diametri: 219,1 mm -3048 mm

Devor qalinligi: 5.0mm-25.4mm

Uzunligi 70 metrgacha

Chelik darajasi

Amerika neft instituti 5L: A darajasi, B darajasi, X42, X46, X56, X60, X65, X70

Amerika ASTM A252 1-darajali, 2-daraja, 3-daraja

ASTM A53: A darajasi, B darajasi, C darajasi, D darajasi

BS 4360: 43-daraja, 50-daraja

UZ: S275, S275jr, S355jrh, S355j2h

Yuzaki ishlov berish: sinterlangan epoksi qoplamasi, ko'mir smolali epoksi qoplamasi, 3PE qoplamasi, xira qoplama, asfalt qoplamasi, qora yog'li qoplama, mijozlar talablariga muvofiq ta'minlanishi mumkin.

XUSUSIYATLAR WWA C 200
MINIMAL MEXANIK XUSUSIYATLAR
PO'lat NARASI Uzilish kuchi, min Ksi
(Mpa)
Oqim chegarasi, min Ksi (Mpa) 2 dyuymga cho'zing
(50 mm)% min

ASTM A-570 / A-570 M gr 30

49 (340) 30 (205) 25 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 33

52 (360) 33 (230) 23 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 36

53 (365) 36 (250) 22 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 40

55 (380) 40 (275) 21 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 45

60 (415) 45 (310) 19 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 50

65 (450) 50 (345) 17 (6 * 2,5 mm)

ASTM A-570 / A-570 M gr 55

70 (480) 55 (380) 15 (6 * 2,5 mm)

ASTM A-36 / A-36 M

58-80 (400-550) 36 (250) 23

ASTM A-283 / A-283 M gr C

55-75 (380-515) 30 (205) 25

ASTM A-283 / A-283 M gr D

60-80 (415-550) 33 (230) 23
  • Spiral payvandlangan po'lat quvurning maksimal diametri AWWA C200, ASTM A139 va ASTM A252 uchun 144 dyuym (3600 mm) ni tashkil qiladi.
  • Quvur devorining qalinligi 1 dyuymgacha
  • 70,000 psi gacha ruxsat etilgan rentabellik
  • Deyarli cheksiz qo'shma yoki tana konfiguratsiyasini qo'llab-quvvatlash uchun armatura va tuzilmalar
  • Dala payvandlash va kauchuk mat qo'shimchalari
  • Payvand choki qo'shma konfiguratsiyalar va mashinaning qirrali uchlari mavjud
  • AWWA C200 va ASTM A139 55 '(nominal) gacha bo'lgan qo'shma uzunliklarda mavjud; ASTM A252 80 'gacha bo'lgan qo'shma uzunliklarda mavjud
  • Astar - suv ta'minoti

AWWA C205 uchun tsement ohak
AWWA C210 uchun epoksi qatroni
AWWA C222 bilan mos keladigan poliuretan

  • Astar - Kanalizatsiya xizmati

Ceramaline® kanalizatsiya qoplamasi
AWWA C222 uchun poliuretan

  • Qoplama - tashqi

Epoksi qatroni (AWWA C210 bilan mos keladi
AWWA C222 bilan mos keladigan poliuretan
AWWA C214 standarti bo'yicha lenta o'rash tizimi

SSAW AWWA C200 quvuri

AWWA C200 welded pipesaw pipe

Issiq teglar: awwa c200 spiral po'lat quvur, Xitoy awwa c200 spiral po'lat quvur ishlab chiqaruvchilari, etkazib beruvchilar

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov