ASTM A135 Gr.B ERW quvurlari
A135 - qarshilik payvandlangan nominal po'lat quvur uchun standart spetsifikatsiya
So'rov yuborish
Hozir chat
Mahsulotni tanishtirish
Qarshilik payvandlangan quvur - payvandlash qismlari yig'ilgandan so'ng elektrodlar orqali bosim o'tkazish va qo'shma va qo'shni joylarning aloqa yuzasi orqali o'tadigan oqim tomonidan ishlab chiqarilgan qarshilik issiqligi yordamida payvandlangan po'lat quvur.
ASTM A135 spetsifikatsiyasi
| Material: | ASTM A135 GRA GRB | Turi: | Elektr qarshilik payvandlangan po'lat quvur |
|---|---|---|---|
| Tashqi diametri: | 5 - 420 mm | Ishlab chiqarish texnologiyasi: | Sovuq chizilgan / sovuq haddelenmiş / issiq haddelenmiş |
| Yuzaki ishlov berish: | Qora lak bilan bo'yalgan, moyli bo'yalgan, galvanizli | Qotishma yoki yo'q: | Qotishma emas |
ASTM A135 ERW quvurining kimyoviy tarkibi
| Element | Tarkibi, maksimal, % | |
| A sinf | B sinf | |
| C | 0.25 | 0.30 |
| Mn | 0.95 | 1.20 |
| P | 0.035 | 0.035 |
| S | 0.035 | 0.035 |
ASTM A135 payvandlangan quvurning mexanik xususiyati
| ASTM A135 | A sinf | B sinf |
|---|---|---|
| Mustahkamlik chegarasi, min, ksi [MPa] |
48 [330] |
60 [415] |
| Hosildorlik kuchi, min, ksi [MPa] |
30 [205] |
35 [240] |
| cho'zilish, min, % |
35 | 30 |
Quvurlar devorining qalinligi bardoshlik jadvali
| Nominal Devor qalinligi |
Nominal OD 22 mm orqali ±mm |
Nominal OD 22-48mm ±mm |
Nominal OD 48-100mm ±mm |
||||
| 0.89 | 0.05/0.05 | 0.05/0.05 | 0.05/0.05 | ||||
| 1.00 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 1.25 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 1.50 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 1.65 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 2.00 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 2.11 | 0.05/0.05 | 0.05/0.08 | 0.05/0.08 | ||||
| 2.410 | 0.05/0.05 | 0.05/0.08 | 0.08/0.08 | ||||
| 2.500 | 0.05/0.08 | 0.05/0.10 | 0.08/0.08 | ||||
| 2.770 | 0.05/0.08 | 0.05/0.10 | 0.08/0.08 | ||||
| 3.000 | 0.05/0.08 | 0.05/0.10 | 0.08/0.08 | ||||
| 3.050 | 0.05/0.08 | 0.05/0.10 | 0.08/0.08 | ||||
| 3.40 | - | 0.05/0.10 | 0.08/0.08 | ||||
| 3.75 | - | 0.05/0.10 | 0.08/0.08 | ||||
| 4.00 | - | 0.08/0.10 | 0.08/0.10 | ||||
| 4.19 | - | 0.08/0.10 | 0.08/0.10 | ||||
| 4.57 | - | 0.10/0.10 | 0.08/0.13 | ||||
| 5.00 | - | 0.10/0.13 | 0.10/0.13 |