Standart: St 37.0 St35.8
Tashqi o'lchamlari: 4 dan 6 mm gacha
Devor qalinligi: 0,5 dan 8 mm gacha
Maksimal uzunlik: 6000 mm
So'rov yuborish
Hozir chat
Mahsulotni tanishtirish

ST37.0 ST35.8 Payvandlangan po'lat quvurlarni yetkazib beruvchi-GNEE

St37.0 St35.8 quvurining tavsifi

St 37.0 ST 35.8 ERW (qarshilik payvandlangan) trubkasi uzunlamasına payvandlanadi va 24 dyuym OD gacha bo'lgan chiziqdan / lasandan tayyorlanadi. St 37.0 ST 35.8 toifali quvur va quvurlar arzon{6}}xarajatsiz, past{7}}uglerodli po‘lat quvur bo‘lib, uglerod miqdori 017% bo‘lib, uni shakllantirish oson.

GNEE Group St37.0 St35.8 payvandlangan quvurlarni ishlab chiqarish va yetkazib berishga ixtisoslashgan, agar sizga kerak bo'lsa, istalgan vaqtda biz bilan bog'lanishingiz mumkin.

St37.0 St35.8 payvandlangan po'lat quvur spetsifikatsiyasi

Kelib chiqqan joyi Xitoy
Brend nomi GNEE
Sertifikatlash ISO Idoralar
Model raqami ST37.0, ST35.8, St37.2, St35.4
Minimal buyurtma miqdori 30 Ton
Narxi Tonna uchun 620 - 780 AQSH dollari
Qadoqlash tafsilotlari yog'och quti yoki mijozning talabiga binoan
Yetkazib berish vaqti 30 kun
To'lov shartlari T/TL/C Western Union MoneyGram
Ta'minot qobiliyati Yiliga 2 000 000 tonna

St37.0 St35.8 karbonli po'lat quvurining standart uzunlikdagi toleranslari

Komponent uzunligi (mm) OD 30-100 mm OD 100-254 mm
10-100 + 1.0/- 0 + 2.0/- 0
100-600 + 2.0/- 0 + 3.0/- 0
600-1200 + 3.0/- 0 + 4.0/- 0
1200-5000 + 5.0/- 0 + 6.0/- 0
Chelik darajasi belgisi Devor qalinligi uchun yuqori rentabellikdagi kuchlanish ReH, mm Kuchlanish kuchi Rm A5 sinishidan keyin cho'zilish Ta'sir kuchi ko'ndalang
ReH£ 16 16< ReH£40 40< ReH£60 Uzunlamasına Transvers
Min N/mm2 Min % Min J
St 37.0 235 225 215 350(1) -480 25 23 -
St 35.8 235 225 215 360-480 25 23 34

St37.0 St35.8 Karbonli po'lat quvur o'lchamlari

Diametrning belgilanishi O/D Nominal devor qalinligi
IIV SCH.5S SCH.5 SCH 10S SCH.10 SCH.20S SCH.30 SCH.40S SCH.40 SCH 60
(A) (B) Metr
MM
Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr Devor
Thk
Og'irligi Kg/Mtr
6 1/8 10.3 1 0.23     1.2 0.27     1.5 0.33     1.73 0.37        
8 1/4 13.7 1.2 0.37     1.65 0.49     2 0.58     2.24 0.64        
10 3/8 17.2 1.2 0.47     1.65 0.63     2 0.74     2.31 0.87        
15 1/2 21.3 1.65 0.01 1.65 0.81 2.11 1.02 2.11 1.02 2.5 1.15     2.77 1.29        
20 3/4 26.7 1.65 1.03 1.65 1.03 2.11 1.3 2.11 1.3 2.5 1.49     2.87 1.71        
25 1 33.4 1.65 1.31 1.65 1.31 2.77 2.13 2.77 2.13 3 2.24     3.38 2.54        
32 11/4 24.2 1.65 1.67 1.65 1.67 2.77 2.73 2.77 2.73 3 2.9     3.56 3.44        
40 11/2 48.3 1.65 1.93 1.65 1.93 2.77 3.16 2.77 3.16 3 3.35     3.68 4.11        
50 2 60.3 1.65 1.93 1.65 2.42 2.77 3.99 2.77 3.99 3.5 4.9     3.91 5.52        
65 21/2 73 2.11 3.75 2.11 3.75 3.05 5.34 3.05 5.34 3.5 6     5.16 8.77        
80 3 88.9 2.11 4.59 2.11 4.59 3.05 6.56 3.05 6.56 4 8.37     5.49 11.47        
90 31/2 101.6 2.11 5.25 2.11 5.25 3.05 7.53 3.05 7.53 4 9.62     5.74 13.78        
100 4 114.3 2.11 5.93 2.11 5.93 3.05 8.5 3.05 8.5 4.5 12.18     6.02 6.32        
125 5 141.3 2.77 9.61 2.77 9.61 3.4 11.74 3.43 11.74 5 16.8     6.55 2210        
150 6 168.3 2.77 11.47 2.77 11.47 3.4 14.04 3.43 14.04 5.5 22.08     7.11 28.69        
200 8 219.1 2.77 15 2.77 15 3.76 20.77 3.76 20.27 6.35 33.82 7.04 37.38 8.18 43.2     10.81 53.9
250 10 273.1 3.4 22.95 3.4 22.95 4.19 28.2 4.19 28.2 6.35 42.41 7.8 51.81 9.27 61.22     12.2 82.8
300 12 323.9 3.96 31.72 4.19 33.6 4.57 36.54 4.57 36.54 6.35 50.48 8.38 66.2 9.53 75.01 10.31 80.94 14.27 110.62
350 14 355.6 3.96 34.86     4.78 41.99 6.35 55.53 7.92 68.95 9.53 82.58 9.53 82.58 11.13 96 15.06 128.42
400 16 406.4 4.19 42.2     4.78 48.07 6.35 63.61 7.92 79.03 9.53 94.7 9.53 94.7 12.7 125.2 16.66 162.59
450 18 457.2 4.19 47.46     4.78 54.15 6.35 71.69 7.92 89.1 11.13 124.32 9.53 106.83 14.27 158.27 19.05 209
500 2C 508 4.78 60.23     5.54 69.7 6.35 79.76 9.53 118.93 12.7 157.51 9.53 118.9 15.06 185.89 2062 251.65
550 22 558.8 4.78 65.95     5.54 76.75 6.35 87.84 9.53 131.07 12.7 173.66 9.53 131.07 15.88 216.04 22.23 298.55
600 24 609.6 5.54 83.8     6.35 95.92 6.35 95.92 9.53 143.2 14.27 212.72 9.53 143.2 17.45 258.74 24.59 360.21
650 26 660.4             7.92 129.4 12.7 205.97     9.53 155.32        
700 28 711.2             7.92 139.47 12.7 222.13 15.88 276.48 9.53 167.44        
750 3C 762 6.35 120.15     7.92 149.55 7.92 149.55 12.7 238.28 15.88 296.68 9.53 179.56        
800 32 812.8             7.92 159.62 12.7 254.44 15.88 316.88 9.53 191.69 17.48 348.11    
850 34 863.6             7.92 169.64 12.7 270.5 15.88 336.96 9.53 203.74 17.48 370.22    
900 36 914.4             7.92 179.77 12.7 286.75 15.88 357.28 9.53 215.93 19.05 427.09  

ST37.0 ST35.8 ERW Chelik quvurlari ko'rgazmasi

ST37.0 ST35.8 hollow steel pipelsaw steel pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Biz haqimizda

GNEE Group ilmiy-tadqiqot, ishlab chiqarish va eksportni birlashtirgan zamonaviy po'lat yetkazib berish zanjiri guruhidir. Ro'yxatdan o'tgan kapitali 60 million RMB bo'lgan kompaniya 100 akrdan ortiq maydonni o'z ichiga oladi, bino maydoni 35 000 kvadrat metr va 200 dan ortiq xodimlar. Kompaniya ilg'or ishlab chiqarish uskunalari va yetuk texnologiyaga ega, ammo yuqori-sifatli professional boshqaruv va texnik xodimlarga ega. Kompaniya xalqaro sifat menejmenti tizimi ISO9001:2000 sertifikatidan o'tdi. Agar sizga po'lat buyumlar kerak bo'lsa, siz o'zingizning maxsus mahsulot talablaringizni ta'minlay olasiz va biz sizga imkon qadar tezroq taklif qilamiz.

GNEE jamoasi shousi

ST35.8 ST37.0 ERW Pipe Supplier

GNEE mijozlari

St 35.8 erw pipe customers

GNEE ko'rgazmasi

carbon pipe exhibition

Payvandlangan quvur sinovi

welded carbon pipe inspection

Qadoqlash va jo'natish

packaging and shipping

Issiq teglar: st37.0 st35.8 erw trubkasi, Xitoy st37.0 st35.8 erw quvur ishlab chiqaruvchilari, etkazib beruvchilari

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov