API 5L X42 X46 X52 payvandlangan quvur
, PSL1 yoki PSL2
,Diametrlari: 1/2" dan 60" gacha.
,Devor qalinligi shkalasi: SCH 10, SCH 40, SCH 80 dan SCH 160
,Qoplamalar: 3PE, FBE, qora, bo'yalgan
, Uzunlik diapazoni: 20 fut (6M), 40 fut (12M)
Professional payvandlangan quvurlar yetkazib beruvchi --GNEE
Mahsulotlar tavsifi
API 5L X42 trubkasi, shuningdek, L290 trubkasi (ISO 3183 bo'yicha) sifatida ham tanilgan, 42,100 Psi yoki 290 Mpa minimal rentabellik kuchi tufayli nomlangan. Bu B dan yuqori nav. API 5L X100 gacha bo'lgan turli navlarga ega, shuning uchun x42 trubkasi past va o'rta navlarga ega va ko'pchilik neft va gaz uzatish quvurlarida ko'p miqdorda talab qilinadi.GNEE API 5L X42/L290 payvandlangan ERW va HFW, LSAW. mahsulot spetsifikatsiyalari PSL1 va PSL2 boʻlib, oʻlchamlari odatdagi 4-dyuym, 6-dyuym, 8-dyuym, 10-dyuym, 12-dyuym, { {20}}dyuym, 20-dyuym 60 dyuymgacha.
API 5L X46 trubkasi API 5L standart spetsifikatsiyasida past va o'rta diapazondagi quvur materialidir. Minimal oqish quvvati 320 Mpa (46,400 psi) bo'lganligi sababli L320 trubkasi sifatida ham tanilgan. Minimal valentlik kuchi 435 Mpa.API 5L X46 choksiz va payvandlangan (ERW, SAW) ishlab chiqarish turlarini qamrab oladi, ikkalasi ham neft va gaz uzatish uchun mos keladi. U ikkita mahsulot spetsifikatsiyasi darajasi PSL1, PSL2ni o'z ichiga oladi. (PSL2 da nordon xizmat uchun materialni o'z ichiga oladi)
API 5L X52 trubkasi L360 trubkasi sifatida ham tanilgan, X52 (L360) 52 Ksi (360 Mpa) minimal rentabellikdan kelib chiqqan holda nomlangan. Bu neft va gaz quvurlarini uzatish uchun API 5L va ISO 3183 spetsifikatsiyalarida oraliq daraja hisoblanadi.
Sanoatning etakchi payvandlangan quvurlarni ishlab chiqarish texnologiyasi


API 5L payvandlangan quvur o'lchamlari
| NB | DN | OD (dyuym) | Jadval | ||||||||||
| Sh 5 | Sh 10 | Sh 20 | Sh 30 | Sh 40 | Sh 60 | Sh 80 | Sh 100 | Sh 120 | Sh 160 | ||||
| 3/4" | 20 | 1.05 | 0.065 | 0.11 | x | 0.095 | 0.113 | x | x | 0.17 | x | 0.219 | |
| 1" | 25 | 1.315 | 0.065 | 0.11 | x | 0.114 | 0.133 | x | x | 0.2 | x | 0.25 | |
| 1.1/2" | 40 | 1.9 | 0.065 | 0.11 | x | 0.125 | 0.145 | x | x | 0.225 | x | 0.281 | |
| 2" | 50 | 2.375 | 0.065 | 0.12 | x | x | 0.154 | x | x | 0.25 | x | 0.344 | |
| 2.1/2" | 65 | 2.875 | 0.083 | 0.12 | x | x | 0.203 | x | x | 0.3 | x | 0.375 | |
| 3" | 80 | 3.5 | 0.083 | 0.12 | x | x | 0.216 | x | x | 0.35 | x | 0.438 | |
| 4" | 100 | 4.5 | 0.083 | 0.12 | x | x | 0.237 | x | x | 0.437 | x | 0.531 | |
| 5" | 125 | 5.563 | 0.109 | 0.12 | x | x | 0.258 | x | x | 0.5 | x | 0.625 | |
| 6" | 150 | 6.625 | 0.109 | 0.13 | x | x | 0.28 | x | x | 0.562 | x | 0.719 | |
| 8" | 200 | 8.625 | 0.109 | 0.15 | 0.25 | 0.277 | 0.322 | 0.406 | 0.593 | 0.718 | 0.812 | 0.906 | |
| 10" | 250 | 10.75 | 0.134 | 0.17 | 0.25 | 0.307 | 0.365 | 0.5 | 0.718 | 0.843 | 1.0 | 1.125 | |
| 12" | 300 | 12.75 | 0.165 | 0.18 | 0.25 | 0.33 | 0.406 | 0.5 | 0.843 | 1.0 | 1.125 | 1.312 | |
ERW Steel Pipe API 5L Mexanik quvvat
| Quvurlar darajasi | Uzatilish xususiyatlari - SMLS va payvandlangan quvurlarning ERW quvur korpusi PSL 1 | ERW payvandlangan trubaning tikuvi | ||
|---|---|---|---|---|
| Hosildorlik kuchi a | Kuchlanish kuchi a | Cho'zilish | Kuchlanish kuchi b | |
| Rt% 7b{0}},5 PSI Min | Rm PSI Min | (2 dyuym Af % min) | Rm PSI Min | |
| A | 30,500 | 48,600 | c | 48,600 |
| B | 35,500 | 60,200 | c | 60,200 |
| X42 | 42,100 | 60,200 | c | 60,200 |
| X46 | 46,400 | 63,100 | c | 63,100 |
| X52 | 52,200 | 66,700 | c | 66,700 |
| X56 | 56,600 | 71,100 | c | 71,100 |
| X60 | 60,200 | 75,400 | c | 75,400 |
| X65 | 65,300 | 77,500 | c | 77,500 |
| X70 | 70,300 | 82,700 | c | 82,700 |
Vaqt sinovidan o'tgan yuqori sifatli payvandlangan quvurlar

Test talablari
Gidrostatik sinov: 100% gidrostatik sinov, payvand choklari yoki quvur tanasidan oqish yo'q. Agar ishlatilgan quvur qismi muvaffaqiyatli sinovdan o'tgan bo'lsa, ulanishlar yoki bo'g'inlar gidrostatik sinovdan o'tkazilishi shart emas.
BEND TEST: Namunaning biron bir qismida yoriqlar yoki payvand teshiklari bo'lmasligi kerak.
Yassilash testi: tekislash testi deformatsiya ostida quvurning ishlashini tekshirish uchun ishlatiladi. U uzunlamasına yorilish va aylana yorilishiga, shu jumladan ichki va tashqi nuqsonlarga qarshilik ko'rsatishi kerak.
Diametri 12,75 dyuymdan ortiq ERW trubkasi uchun;
Quvurlar > 10 OD/wt uchun, plitalar orasidagi masofa asl ODning 30% dan kam bo'lmaguncha payvand choklarida teshiklar bo'lmasligi kerak.
Yo'naltirilgan egilish testi: to'liq sinish; chuqurligidan qat'i nazar, uzunligi 3,2 mm dan ortiq bo'lgan chok metallida har qanday yoriq yoki yoriqni ko'rsatish. yoki asosiy metall, issiqlik ta'sir zonasi yoki termoyadroviy chiziqdagi devor qalinligidan 3,2 mm dan ortiq uzunlikni yoki 12,5% dan ortiq chuqurlikni ochib beradi.
CVN ta'sir sinovi: (PSL2 trubkasi uchun talab qilinadi, choksiz quvur uchun sinov quvur tanasi bilan, payvandlangan sinov uchun, shu jumladan quvur tanasi, payvand va issiqlik ta'sir zonasi HAZ testi uchun) DWT testi: (PSL2 trubkasi uchun talab qilinadi)
Issiq teglar: api 5l x42 x46 x52 payvandlangan quvur, Xitoy api 5l x42 x46 x52 payvandlangan quvur ishlab chiqaruvchilari, etkazib beruvchilari
Keyingi2
API 5L B darajali quvurSizga ham yoqishi mumkin
So'rov yuborish