DIN1626 ST37 To'g'ri tikuv trubkasi
ST37 uglerod quvurlari asosan issiq va sovuq haddeleme bilan qayta ishlanadi. Po'lat quvur yaxshi qoliplash xususiyatlariga ega bo'lgani uchun u mijozlarning turli ehtiyojlarini qondirishi mumkin. Bunga qo'shimcha ravishda, past uglerod miqdori ham ushbu sinfni payvandlashni juda osonlashtiradi. din 2391 st 37 uglerodli po'lat quvurlari yuqori bosimli ilovalarni engish uchun turli bosim sinflari va o'lchagichlarda mavjud.
ST37 po'lat choksiz quvurining kimyoviy tarkibi
| C | N | P | S |
| 0.21-0.25 | 0.009 | 0.065 | 0.065 |
St37 uglerod quvurlariSpetsifikatsiya
| Standart | DIN 1626 |
| Baho | OʻT |
| Hajmi | OD ({0}}mm) x VT (0.5-15mm) |
| Tashqi o'lchamlar | 4.0mm – 60,0mm |
| Devor qalinligi | 0.5 mm – 8 mm |
| Uzunlik | Maksimal 6000 mm |
ST37 quvurlarga chidamlilik
|
OD tolerantligi |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
% 7b% 7b0}% 7dmm |
|
±0,08 mm |
±0,15 mm |
±0.20mm |
±0,25 mm |
±0.30mm |
±0.30mm |
±0.40mm |
±0,45 mm |
|
|
WT tolerantligi |
±10% |
|||||||
DIN 2391 ST37 Karbonli po'lat quvurlari o'lchamlari
| Devor | O'lchamlar (OD) |
| .010 | 1/16″ , 1/8″ , 3/16″ |
| .020 | 1/16″ , 1/8″ , 3/16″ , 1/4″ , 5/16″ , 3/8″ |
| .012 | 1/8″ |
| .016 | 1/8″ , 3/16″ |
| .028 | 1/8″ , 3/16″ , 1/4″ , 5/16″ , 3/8″ , 1/2″ , 3/4″ , 1″ , 1 1/2″ , 2″ |
| .035 | 1/8″ , 3/16″ , 1/4″ , 5/16″ , 3/8″ , 7/16″ , 1/2″ , 16″ , 5/8″ , 3/4″ , 7/8″ , 1″ , 1 1/4″ , 1 1/2″ , 1 5/8″ , 2″ , 2 1/4″ |
| .049 | 3/16″ , 1/4″ , 5/16″ , 3/8″ , 1/2″ , 16″ , 5/8″ , 3/4″ , 7/8″ , 1″ , 1 1/8″ , 1 1/4″ , 1 1/2″ , 1 5/8″ , 2″ , 2 1/4″ |
| .065 | 1/4″ , 5/16″ , 3/8″ , 1/2″ , 16″ , 5/8″ , 3/4″ , 7/8″ , 1″ , 1 1/4″ , 1 1/2″ , 1 5/8″ , 1 3/4″ , 2″ , 2 1/2″ , 3″ |
| .083 | 1/4″ , 3/8″ , 1/2″ , 5/8″ , 3/4″ , 7/8″ , 1″ , 1 1/4″ , 1 1/2″ , 1 5/8″ , 1 7/8″ , 2″ , 2 1/2″ ,3″ |
| .095 | 1/2″ , 5/8″ , 1″ , 1 1/4″ , 1 1/2″ , 2″ |
| .109 | 1/2″ , 3/4″ , 1″ , 1 1/4″ , 1 1/2″ , 2″ |
| .120 | 1/2″ , 5/8″ , 3/4″ , 7/8″ , 1″ , 1 1/4″ , 1 1/2″ , 2″ , 2 1/4″ , 2 1/2″ , 3″ |
| .125 | 3/4″ , 1″ , 1 1/4″ , 1 1/2″ , 2″ , 3″ , 3 1/4″ |
| .134 | 1″ |
| .250 | 3″ |
| .375 | 3 1/2″ |
DIN1626 ST37 To'g'ri tikuv trubkasi


Issiq teglar: din1626 st37 tekis tikuv trubkasi, Xitoy din1626 st37 tekis tikuv trubkasi ishlab chiqaruvchilari, etkazib beruvchilari
Keyingi2