Q345 Q235 payvandlangan po'lat quvur
Past qotishma konstruktiv po'lat sifatida q345 mukammal mexanik xususiyatlarga ega, past haroratlarga bardosh bera oladi va yaxshi plastiklikka ega. Shuning uchun, bu po'latdan Shanxay Pudong xalqaro aeroporti qurilishi, Jiujiang Yangtze daryosi ko'prigi qurilishi kabi yirik binolar, avtomobil yo'llari ko'prigi, yuqori bosimli idishlar, payvandlangan metall konstruktsiyalar va boshqalarda foydalanish mumkin.
Q345 payvandlangan po'lat quvur kimyoviy elementlar jadvali
| Turi | Kimyoviy element | |
| q345 | a | C {0}} dan kichik yoki teng.20,Mn 1,70 dan kichik yoki teng,Si 0,50 dan kichik yoki teng,P dan kichik yoki teng 0,035,S 0,035 dan kam yoki teng |
| b | C {0}} dan kichik yoki teng.20,Mn 1,70 dan kichik yoki teng,Si 0,50 dan kichik yoki teng,P dan kichik yoki teng 0,035,S 0,035 dan kam yoki teng | |
| c | C {0}} dan kichik yoki teng,20,Mn 1,70 dan kichik yoki teng,Si 0.50 dan kichik yoki teng, P 0,030 dan kichik yoki teng, S 0,030 dan kichik yoki teng, Al 0,015 dan katta yoki teng | |
| d | C {0}} dan kichik yoki teng.18,Mn 1,7 dan kichik yoki unga teng0,Si 0 dan kichik yoki teng.50, P 0,030 dan kichik yoki teng, S 0,025 dan kichik yoki teng, Al 0,015 dan katta yoki teng | |
| e | C {0}} dan kichik yoki teng.18,Mn 1,7 dan kichik yoki unga teng0,Si 0 dan kichik yoki teng.50, P 0,025 dan kichik yoki teng, S 0,020 dan kichik yoki teng, Al 0,015 dan katta yoki teng |
Q345 ERW payvandlangan po'lat quvur

Q235 - uglerodli po'latdir, odatda past quvvat talablari bo'lgan qismlarni karbürleme yoki siyanidlash uchun ishlatiladi, bog'lovchi novdalar, bog'lovchi novdalar, ilgaklar, muftalar, murvat va yong'oqlar, yenglar, miller va payvandlar.
Q235 karbonli po'latdan kimyoviy elementlar jadvali
| Turi | Kimyoviy element | |
| q235 | A |
C {0}} dan kichik yoki teng.22% Mn 1,4% dan kam yoki teng Si 0 dan kichik yoki teng.35% S {{8} dan kichik yoki teng },050 P 0,045 dan kam yoki unga teng |
| B | C {0}} dan kichik yoki teng.20% Mn 1,4% dan kam yoki teng Si 0 dan kichik yoki teng.35% S dan kichik yoki teng 0,045 P gacha 0,045 dan kam yoki teng | |
| C | C {0}} dan kichik yoki teng.17% Mn 1,4% dan kam yoki teng Si 0 dan kichik yoki teng.35% S {{8} dan kichik yoki teng },040 P 0,040 dan kam yoki unga teng | |
| D | C {0}} dan kichik yoki teng.17% Mn 1,4% dan kam yoki teng Si 0 dan kichik yoki teng.35% S {{8} dan kichik yoki teng },035 P 0,035 dan kam yoki unga teng |
Q345 Q235 po'lat quvur hajmi
| Turi |
Hajmi |
| q345 q235 | 600*600*(8.0-30) |
| 550*550*(8.0-25) | |
| 500*500*(8.0-25) | |
| 450*450*(8.0-20) | |
| 420*420*(8.0-20) | |
| 400*400*(8.0-20) | |
| 380*380*(6.0-20) | |
| 350*350*(6.0-20) | |
| 320*320*(6.0-20) | |
| 300*300*(6.0-16) | |
| 280*280*(8.0-16) | |
| 250*250*(6.0-16) | |
| 220*220*(3.75-14) | |
| 200*200*(3.75-14) | |
| 180*180*(5.0-12) | |
| 160*160*(3.0-12) | |
| 150*150*(3.0-12) | |
|
140*140*(3.75-12) |
|
|
130*130*(3.0-12) |
|
|
120*120*(3.0-12) |
|
|
100*100*(2.0-12) |
|
|
90*90*(3.0-6.0) |
|
| 80*80*(1.5-8.0) | |
| 75*75*(2.0-6.0) | |
|
70*70*(2.0-6.0) |
|
| 60*60*(1.2-6.0) | |
|
50*50*(1.0-5.0) |
|
|
40*40*(0.8-4.5) |
|
| 35*35*(0.8-3.0) | |
|
30*30*(0.8-3.0) |
|
| 25*25*(0.8-2.5) | |
|
20*20*(0.8-2.5) |
|
|
19*19*(0.8-1.5) |
|
|
15*15*(0.5-1.5) |
Bizning afzalliklarimiz
Pastroq narxlar: Bizni tanlang va siz ko'proq xarajatlarni tejaysiz.
Yaxshiroq xizmat: Bizni tanlang, siz yanada keng qamrovli xizmat sifatiga ega bo'lasiz.
Ko'proq ajoyib qadoqlash: Bizni tanlang, tovarlar sizning oldingizda eng mukammal holatda bo'ladi.
Qisqaroq javob vaqti: Biz sizning so'rovingizga 24 soat ichida javob beramiz.
Qisqaroq yetkazib berish muddati: Buyurtmangizni o'z vaqtida ishlatishingiz uchun 7 kun ichida jo'natamiz.
Yaxshiroq sotishdan keyingi xizmat: Agar sizda muammo bo'lsa, biz siz uchun hal qilishga tayyormiz.
GNEE haqida
GNEE GROUP po'lat, metallurgiya, mashinasozlik va boshqa sanoat tarmoqlariga ega bo'lgan keng qamrovli po'lat yetkazib berish zanjiri korxonasidir. Guruhning eng yirik sho''ba korxonasi sifatida Chelik bo'limi FDA, CCS, ABS va RINA kabi bir qator texnik sertifikatlarga ega. Biz dunyoning ko'plab mintaqalari va mamlakatlaridagi korxonalar bilan hamkorlik qildik va turli xil po'lat mahsulotlari Osiyo Tinch okeani, Evropa va Amerikaga eksport qilinmoqda.



Issiq teglar: q345 q235 payvandlangan po'lat quvur, Xitoy q345 q235 payvandlangan po'lat quvur ishlab chiqaruvchilari, etkazib beruvchilari
Oldingi
qotishma payvandlangan quvurKeyingi2
API 5L X42 tikuvli po'lat quvurSizga ham yoqishi mumkin