1. Kimyoviy tarkibini taqqoslash
| Element | ASTM A139 | ASTM A252 (Gr.3) |
|---|---|---|
| Uglerod (C) | 0,26% dan kam yoki unga teng | 0,26% dan kam yoki unga teng |
| Marganets (Mn) | 1,20% dan kam yoki unga teng | 1,20% dan kam yoki unga teng |
| Fosfor (P) | 0,05% dan kam yoki unga teng | 0,05% dan kam yoki unga teng |
| Oltingugurt (S) | 0,05% dan kam yoki unga teng | 0,05% dan kam yoki unga teng |
| Kremniy (Si) | 0,20% dan kam yoki unga teng | 0,20% dan kam yoki unga teng |
2. Mexanik xususiyatlarni taqqoslash
| Parametr | ASTM A139 | ASTM A252 (Gr.3) |
|---|---|---|
| Hosildorlik kuchi | 240 MPa dan katta yoki unga teng | 241 MPa dan katta yoki unga teng |
| Mustahkamlik chegarasi | 415 MPa dan katta yoki unga teng | 455 MPa dan katta yoki unga teng |
| Cho'zilish | 24% dan katta yoki teng | 20% dan katta yoki teng |
3. Mexanik ishlashni taqqoslash
| Xarakterli | ASTM A139 | ASTM A252 |
|---|---|---|
| To'g'rilik talabi | Maxsus talab yo'q | Uzunlikning 0,25% dan kam yoki unga teng |
| Tekshirish standarti | 100% gidrostatik sinov | 100% payvandlash tekshiruvi |
| Harorat diapazoni | -30 daraja ~+80 daraja | -20 daraja ~+50 daraja |
4. Ilovadagi farqlar
ASTM A139Suyuqlik uzatish quvurlari, qurilish konstruktiv tayanchlari, mexanik ishlab chiqarish
ASTM A252Qoziq poydevori muhandisligi, qazishni qo'llab-quvvatlash, port terminali inshootlari
A252 qoziq quvurlari zavodi