A358 po'lat quvur yuqori haroratda foydalanish uchun elektrofüzyon bilan payvandlangan ostenitik xrom-nikel qotishma po'lat quvur bo'lib, A312 standartidan ko'ra qattiqroq spetsifikatsiya standartidir.
GNEE Group zanglamaydigan po'latdan yasalgan elektro termoyadroviy payvandlangan quvurlar va quvurlarning professional yetkazib beruvchisi bo'lib, biz 304, 304L, 304H, 309, 309S, 310,310S, 316, 316L, 316H, 3137L, 314H, jumladan, keng turdagi mahsulotlarni yetkazib beramiz. ,904 va boshqalar. Agar kerak bo'lsa, istalgan vaqtda biz bilan bog'lanishingiz mumkin.
A358 EFW quvurining spetsifikatsiyasi
| Standart |
ASTM, DIN, JIS, GB, AISI, ISO va boshqalar xalqaro standartlar |
| O'lchamlari |
ASTM, ASME va API |
| Texnik xususiyatlari |
ASTM A358 / ASME SA 358 - 1-sinf, 3-sinf, 2-sinf, 4-sinf, 5-sinf |
| Baho |
TP 304, TP 304L/H, TP 304LN, TP 316L, TP 316, TP 321/H, TP 347/H |
| Hajmi |
8" NB dan 72" NB gacha. |
| Qalinligi |
3 mm dan 60 mm gacha |
| Uzunlik |
6 metrgacha, maxsus kesilgan uzunliklar |
| Devor qalinligi |
ANSI B36.19/36.10 ga muvofiq 3 mm dan 20 mm gacha, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S |
| Tugatish |
№1 tuzlangan qoplama, BA tugatish, №4 tugatish, elektropolislangan choksiz po'lat quvurlar |
| Yetkazib berish sharti |
Issiq pardozlash, sovuq pardozlash, yorqin tavlangan, tavlangan va tuzlangan, sayqallangan, passivlangan, stressdan xalos bo'lgan |
| Ilova |
Oziq-ovqat va ichimliklar sanoati, yadroviy, qurilish sanoati, issiqlik va elektr stansiyalari, neft-kimyo, qozonxonalar, sement sanoati, geotermal zavodlar, asbobsozlik ishlari, mexanik ishlar, issiqlik almashinuvchilari, neft va gaz uskunalari va quvurlari |
| Paket |
Chelik to'plamlar, ikkala uchida plastik qopqoqlar, to'quv sumkalar yoki so'rov bo'yicha |
A358 zanglamaydigan po'lat quvur kimyoviy tarkibi
| A358 SINFLARI |
BMTTD |
C |
Mn |
P |
S |
Si |
Cr |
Ni |
Moʻy |
Ti |
Nb |
N |
| TP304 |
S3040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304L |
0.035 |
|
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-13.0 |
|
|
|
|
| TP304H |
S30409 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-11.0 |
|
|
|
|
| TP304N |
S30451 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-18.0 |
|
|
|
0.10-0.16 |
| TP304LN |
S30453 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
8.0-12.0 |
|
|
|
0.10-0.16 |
| ASME SA358 TP309S |
S30908 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
0.75 |
|
|
|
| ASME SA358 TP309H |
S30909 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-15.0 |
|
|
|
|
| ASME SA358 TP309Cb |
S30940 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1,10 maks |
|
| ASME SA358 TP309HCb |
S30941 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
22.0-24.0 |
12.0-16.0 |
0.75 |
|
10xC min 1,10 nmax |
|
| ASME SA358 TP310S |
S3108 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
|
|
| ASME SA358 TP310H |
S3109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
|
|
|
|
| ASME SA358 TP310Cb |
S31040 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1,10 maks |
|
| ASME SA358 TP310HCb |
S31041 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
24.0-26.0 |
19.0-22.0 |
0.75 |
|
10xC min 1,10 maks |
|
| ASME A358 TP316 |
S3160 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316L |
S31603 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
|
| ASTM SA358 TP316H |
S31609 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
|
| TP316Ti |
S31635 |
0.08 |
2.0 |
0.045 |
0.030 |
0.75 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
5x (C-N) -0.70 |
|
0.10 |
| TP316N |
S31651 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
10.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| TP316LN |
S31653 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
16.0-18.0 |
11.0-14.0 |
2.0-3.0 |
|
|
0.10-0.16 |
| ASME SA358 TP317 |
S3170 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
10.0-14.0 |
3.0-4.0 |
|
|
|
| ASME SA358 TP317L |
S31703 |
0.035 |
2.0 |
0.045 |
0.030 |
1.0 |
18.0-20.0 |
11.0-15.0 |
3.0-4.0 |
|
|
|
| TP321 |
S3210 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP321H |
S32109 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-12.0 |
|
|
|
0.10 |
| TP347 |
S3470 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347H |
S34709 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| TP347LN |
S34751 |
0.05-0.02 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
0.20- 50.0 |
0.06-0.10 |
| TP348 |
S3480 |
0.08 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
| ASME SA358 TP348H |
S34809 |
0.04-0.10 |
2.0 |
0.045 |
0.030 |
1.0 |
17.0-19.0 |
9.0-13.0 |
|
|
|
|
ASME SA358 EFW po'lat quvurlari mexanik xususiyatlari
| Material |
Issiqlik |
Harorat |
Mustahkamlik chegarasi |
Hosildorlik kuchi |
Uzayish %, min |
| Davolash |
Min. |
Ksi (MPa), min. |
Ksi (MPa), min. |
| |
º F(º C) |
|
|
| TP304 |
Yechim |
1900 (1040) |
75(515) |
30(205) |
35 |
| TP304L |
Yechim |
1900 (1040) |
70(485) |
25(170) |
35 |
| TP316 |
Yechim |
1900(1040) |
75(515) |
30(205) |
35 |
| TP316L |
Yechim |
1900(1040) |
70(485) |
25(170) |
35 |
ASTM A358 po'lat quvurlarga chidamlilik
| NPS ko'rsatkichi |
Tashqi diametrdagi ruxsat etilgan o'zgarishlar |
| Over In. |
In ostida. |
| 1/8 dan 1-1/2 gacha, shu jumladan |
1/64 (0.015) |
1/32 (0.031) |
| 1-1/2 dan 4 gacha, shu jumladan |
1/32 (0.031) |
1/32 (0.031) |
| 4 dan 8 gacha, shu jumladan |
1/16 (0.062) |
1/32 (0.031) |
| 8 dan 18 gacha, shu jumladan |
3/23 (0.093) |
1/32 (0.031) |
Nominal devor qalinligi
| NPS ko'rsatkichi |
Tashqi diametri ichkarida. |
Jadval 5S in. |
Jadval 10S in. |
Jadval 40S in. |
Jadval 80S in. |
| 1/4 |
0.540 |
|
0.065 |
0.088 |
0.119 |
| 3/8 |
0.675 |
|
0.065 |
0.091 |
0.126 |
| 1/2 |
0.840 |
0.065 |
0.083 |
0.109 |
0.147 |
| 3/4 |
1.050 |
0.065 |
0.083 |
0.113 |
0.154 |
| 1.0 |
1.315 |
0.065 |
0.109 |
0.133 |
0.179 |
| 1 1/4 |
1.660 |
0.065 |
0.109 |
0.140 |
0.191 |
| 1 1/2 |
1.900 |
0.065 |
0.109 |
0.145 |
0.200 |
| 2 |
2.375 |
0.065 |
0.109 |
0.154 |
0.218 |
| 2 1/2 |
2.875 |
0.083 |
0.120 |
0.203 |
0.276 |
| 3 |
3.500 |
0.083 |
0.120 |
0.216 |
0.300 |
| 3 1/2 |
4.000 |
0.083 |
0.120 |
0.226 |
0.318 |
| 4 |
4.500 |
0.083 |
0.120 |
0.237 |
0.337 |
| 5 |
5.563 |
0.109 |
0.134 |
0.258 |
0.375 |
| 6 |
6.625 |
0.109 |
0.134 |
0.280 |
0.432 |
| 8 |
8.625 |
0.109 |
0.148 |
0.322 |
0.500 |
| 10 |
10.750 |
0.134 |
0.165 |
0.365 |
0.500 |
| 12 |
12.750 |
0.156 |
0.180 |
0.375 |
0.500 |
Devor qalinligi bardoshliligi ASTM A358 po'lat quvur
| NPS |
ASTM A358 po'lat quvurlarga chidamliligi, % |
| + |
– |
| 1/8-2 1 /2 |
20.0 |
12.5 |
| 3~18, t/D 5% dan kam yoki teng |
22.5 |
12.5 |
| 3~18, t/D> 5% |
15.0 |
12.5 |
| 20 dan katta yoki teng, payvandlangan |
17.5 |
12.5 |
| 20 dan katta yoki teng, choksiz, t/D 5% dan kam yoki teng |
22.5 |
12.5 |
| ≥ 20, seamless, t/D> 5% |
15.0 |
12.5 |