ASTM A556 / A556M} Carbon temir ozuqa suvli isitgichlar uchun ASTM A556MM standart spetsifikatsiyasi. Quvurlar asosan u - naychalar shaklida beriladi.

Sinflar: ASTM A556 sinfi A2, B2 sinfi, C2 sinfi

Hajmi:

Tashqi diametri: 12-40mm

Devor qalinligi: 1-4mm

Uzunlik: maksimal uzunlik 27 metr

ASTM A556 kimyo tarkibi%

Baho

C max

Mn

P maxr

S max

A2

0.18

0.27-0.63

0.035

0.035

B2

0.27

0.29-0.93

0.030

0.030

C2

0.30

0.29-1.06

0.030

0.030

ASTM A556 mexanik xususiyatlari

Baho

Mustahkamlik chegarasi

MPA min

Kuch berish kuchi

MPA min

50mm% minut

A2

47 (320)

26(180)

35

B2

60(410)

37(260)

30

C2

70 (480)

40 (280)

30

 

Etakchi qozon va isitgich etkazib beruvchi va ishlab chiqaruvchi va ishlab chiqaruvchi, ASTM A556 po'lat pubdniyasi zavod narxiga ko'tariladi

Issiq teglar: astm a556 Sovuq isitgichlar, Xitoy ASTM A556 ishlab chiqaruvchilar, Astm A556 Omzerater isitgichlari, Astm A556 fabrikasi

关于焊管的优势你了解哪些?_焊接

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov