ASTM A671 CJA115 sinf 71 po'lat quvur

1. ASTM A671 CJA115 sinf 71 po'lat quvur nima?

Javob:
ASTM A671 CJA115 71-sinf - buelektr-fusion{1}}payvandlangan (EFW) karbonli po'lat quvuruchun mo'ljallanganultra-past{1}}harorat xizmati (-50 daraja F/-45 darajagacha)va yuqori{0}}bosimli ilovalar. "71-sinf" aminimal oqish quvvati 71 ksi (490 MPa), uni muhim kriogen va bosim tizimlari uchun mos qilish.


2. Asosiy material xossalari?

Javob:

Mexanik:

Hosildorlik kuchi: 71 ksi (490 MPa) dan katta yoki unga teng.

Kuchlanish kuchi: 82–102 ksi (565–703 MPa).

Ta'sir sinovi: Charpy V-cho'qqisida-50 daraja Fmo'rtlikka chidamliligini ta'minlash.

Kimyoviy:

Uglerod (C): 0,28% dan kam yoki unga teng, Marganets (Mn): 0,95-1,40%, Kam aralashmalar (P/S 0,035% dan kam yoki teng).


3. Odatdagi ilovalar?

Javob:

Asosiy foydalanish:

LNG (suyultirilgan gaz) terminallari va quvurlari.

Kriogen saqlash tanklari (-45 darajali muhit).

Ekstremal iqlim sharoitida yuqori-bosimli gaz uzatilishi.

Sanoat:Neft va gaz, neft-kimyo, energiya.


4. 71-sinf 70 yoki 63-sinf bilan qanday taqqoslanadi?

Javob:

Sinf Hosildorlik kuchi Asosiy afzallik
63-sinf 63 ksi Umumiy past-harorat
70-sinf 70 ksi Yuqori-bosim
71-sinf 71 ksi Kriogen yuklar uchun mustahkamlangan quvvat

5. Ishlab chiqarish va payvandlash talablari?

Javob:

Payvandlash:Sovuq yorilishning oldini olish uchun oldindan qizdirish (250–400 daraja F) + PWHT (-payvanddan keyingi issiqlik bilan ishlov berish) majburiydir.

Sinov:ASTM A671 bo'yicha gidrostatik + buzilmaydigan (RT/UT).

Shakllantirish: Stress relief for cold bending (thickness >1 dyuym/25,4 mm).