ASTM A672 darajasi B60, C65 quvurlari spetsifikatsiyasi
ASTM A672 Amerika Sinov va Materiallar Jamiyati tomonidan ishlab chiqilgan o'rta va yuqori haroratli bosim ilovalari uchun elektr payvandlangan po'lat quvurlar uchun standartdir. B60 va C65 - bu uning moddiy navlari:
B60 darajasi: tejamkor uglerodli marganets po'lati, minimal oqish quvvati 60 ksi (414 MPa)
C65 darajasi: O'rta{1}}yuqori mustahkam uglerodli marganets po'lati, minimal oqish quvvati 65 ksi (450 MPa)
Umumiy ishlab chiqarish jarayonlari: elektrofüzyon payvandlash (EFW) yoki suv ostida payvandlash (SAW)
Majburiy normallashtiruvchi ishlov berish (don hajmini aniqlaydi va yuqori-harorat ish faoliyatini yaxshilaydi)
Sinf (standart CL22: mahalliy buzilmaydigan-test)
ASTM A672 materiali uchun kimyoviy talablar:
| Spetsifikatsiya | Chelik darajasi | Kimyoviy tarkibi | Izohlar | |||||
|---|---|---|---|---|---|---|---|---|
| C | Si | Mn | P | S | Ti | |||
| Bosim xizmati uchun quvurlar ASTM A671, A672 |
-/A45 | -/0.17 | - | 0.98 | 0.035 | 0.035 | - | A671/ A672 |
| -/A50 | -/0.22 | - | ||||||
| CA55/A55 | 0.28 | - | ||||||
| -/B55 | -/0.20 | 0.13 ~0.45 |
||||||
| CB60/B60 | 0.24 | |||||||
| CB65/B65 | 0.28 | |||||||
| CB70/C70 | 0.31 | 1.30 | ||||||
| -/C55 | -/0.18 | 0.55 ~0.98 |
||||||
| CC60/C60 | 0.21 | |||||||
| CC65/C65 | 0.24 | 0.79 ~1.30 |
||||||
| CC70/C70 | 0.27 | |||||||
ASTM A672 payvandlangan quvurlarning mexanik xususiyatlari:
| Mahsulotlar | Chelik darajasi | ASOSIY METAL MEXANIK TARKIBI | Payvandlash nuqtasining kuchlanish kuchi (N/mm2) | Izohlar | |||
|---|---|---|---|---|---|---|---|
| Chiqish nuqtasi (N/mm2) | Kuchlanish kuchi (N/mm2) | Sinov qismlari | Uzayish (%) | ||||
| ASTM A671, A672 bosim xizmati uchun quvurlar | -/A45 | -/165 | -/310~450 | - | -/30 | -/310~450 | A671/ A672 |
| -/A50 | -/185 | -/345~485 | -/28 | -/345~485 | |||
| CA55/A55 | 205 | 380~515 | 27 | 380~515 | |||
| -/B55 | -/205 | -/380~515 | -/27 | -/380~515 | |||
| CB60/B60 | 220 | 415~550 | 25 | 415~550 | |||
| CB65/B65 | 240 | 450~585 | 23 | 450~585 | |||
| CB70/B70 | 260 | 485~620 | 21 | 485~620 | |||
| -/C55 | -/205 | -/380~515 | -/27 | -/380~515 | |||
| CC60/C60 | 220 | 415~550 | 25 | 415~550 | |||
| CC65/C65 | 240 | 450~585 | 23 | 450~585 | |||
| CC70/C70 | 260 | 485~620 | 21 | 485~620 | |||
test talabi
Kuchlanish va egilish sinovlari
Charpy V-Norch testi (nominal devor qalinligi 1/2 dyuym va undan katta quvur uchun)
Qattiqlik sinovi
Mahsulot tahlili
Metallografiya
Asosiy metallning magnit zarrachalarini tekshirish
Payvandlangan metallning magnit zarrachalarini tekshirish
Payvandlangan metallning suyuqlik penetrant tekshiruvi
Yassi plastinaning tekis nurli ultratovush tekshiruvi-UT1
Yassi plastinaning tekis nurli ultratovush tekshiruvi-UT2
Burchak-Nurli ultratovush tekshiruvi (plastinka qalinligi 2 dyuym 50,8 mm dan kam)-UT3
Sinov va tekshirish

Qadoqlash va jo'natish