Germaniya DIN 17175 standarti

Asosan ishlab chiqarilgan po'lat quvur markalari:
St35.8, St45.8, 15Mo3, 13CrMo44, 10CrMo910 va boshqalar.
Muzokaralar natijasida boshqa markadagi po'lat quvurlar ham etkazib berilishi mumkin.

Mexanik xatti-harakatlar:

Standart

Baho

Kuchlanish kuchi (MPa)

Hosildorlik kuchi (MPa)

Uzayish (%)

DIN 17175

St35.8

360-480

235 dan katta yoki teng

25 dan katta yoki teng

St45.8

410-530

255 dan katta yoki teng

21 dan katta yoki teng

15Mo3

450-600

270 dan katta yoki teng

20 dan katta yoki teng

13CrMo44

440-590

290 dan katta yoki teng

20 dan katta yoki teng

10CrMo910

450-600

280 dan katta yoki teng

18 dan katta yoki teng

ST35.8 Boiler Pipe

Kimyoviy tarkibi:

Standart

Baho

Kimyoviy tarkibi

C

Si

Mn

P,S

Cr

Moʻy

DIN 17175

St35.8

0 dan kichik yoki unga teng.17

0.10-0.35

0.40-0.80

0.030 dan kichik yoki unga teng

/

/

St45.8

0 dan kichik yoki unga teng.21

0.10-0.35

0.40-1.20

0.030 dan kichik yoki unga teng

/

/

15Mo3

0.12-0.20

0.10-0.35

0.40-0.80

0.030 dan kichik yoki unga teng

/

0.25-0.35

13CrMo44

0.10-0.18

0.10-0.35

0.40-0.70

0.030 dan kichik yoki unga teng

0.70-1.10

0.45-0.65

10CrMo910

0.08-0.15

0 dan kichik yoki unga teng.50

0.40-0.70

0.030 dan kichik yoki unga teng

2.00-2.50

0.90-1.20

15Mo3 Boiler Pipe 