Jis g3429 yuqori - bosimli gaz tsilindr uchun
JIS B 8230 va JIS B 8241 da ko'rsatilgan "Linun po'latida ko'rsatilgan" Latun po'latida "Latun po'latida" Latun po'latida "Latun po'latida" Latun po'latlari "Sth12 va Sth22-dagi" Docunth Sth22 "bazasiz po'lat pillionlari.
Sint: Sth 11, Sth 12, Sth 21, Sth 22 sth 31
OD: 48 - 711 mm
WT: 3.1 - 38 mm
Uzunlik: 4 - 14 m m
Ilova: Olov - Gighting Gaz ballonlari, sanoat gaz ballonlari, transport vositasi gaz ballonlari
| Standart | Kimyoviy tarkibi | ||||||
| Baho | C | Si | Mn | P,S | Ni | Mor | Kri |
| Sth 11 | 0,50 dan kam yoki teng | 0.10 - 0.35 | 1,80 dan kam yoki teng | 0,035 dan kam yoki unga teng | / | / | / |
| Sth 12 | 0.30 - 0.41 | 0.10 - 0.35 | 1.35 - 1.70 | 0,030 dan kam yoki unga teng | / | / | / |
| Sth 21 | 0.25 - 0.35 | 0.15 - 0.35 | 0.40 - 0.90 | 0,030 dan kam yoki unga teng | 0,25 dan kam yoki unga teng | 0.15 - 0.30 | 0.80 - 1.20 |
| Sth 22 | 0.33 - 0.38 | 0.15 - 0.35 | 0.40 - 0.90 | 0,030 dan kam yoki unga teng | 0,25 dan kam yoki unga teng | 0.15 - 0.30 | 0.80 - 1.20 |
| Sth 31 | 0.35 - 0.40 | 0.10 - 0.50 | 1.20 - 1.50 | 0,030 dan kam yoki unga teng | 0.50 - 1.00 | 0.30 - 0.60 | 0.15 - 0.25 |
Sanoat gaz / yong'inga qarshi ma'lumotlar qo'zg'ash
| Model | Suv sig'imi oralig'i [L] [IN3] |
Tashqi diametri [mm] [ichida] |
Qalinlik [mm] [ichida] |
Xizmatning bosimi [bar] [psio] |
Sinov bosimi [bar] [psio] |
| Ø 267 ~ 275 mm | |||||
| AC055 | 40 ÷ 100 / 2440 ÷ 6102 | 267 / 10,5 | 4,6 / 0,181 | 167 / 2422 | 250 / 3626 |
| AC040 | 40 ÷ 100 / 2440 ÷ 6102 | 267 / 10,5 | 5,5 / 0,217 | 200 / 2901 | 300 / 4351 |
| AD003 | 30 ÷ 100 / 1830 ÷ 6102 | 273 / 10,7 | 7,7 / 0,303 | 300 / 4351 | 450 / 6527 |
| Ø 316 ~ 323 mm | |||||
| AC056 | 50 ÷ 150 / 3051 ÷ 9154 | 316 / 12,4 | 4,0 / 0,157 | 60 / 870 | 90 / 1305 |
| AC070 | 50 ÷ 150 / 3051 ÷ 9154 | 316 / 12,4 | 4,0 / 0,157 | 66 / 957 | 100 / 1450 |
| AC073 | 50 ÷ 150 / 3051 ÷ 9154 | 320 / 12,6 | 4,0 / 0,157 | 200 / 2901 | 300 / 4351 |
| Ø 345 ~ 356 mm | |||||
| AC078 | 60 ÷ 150 / 3661 ÷ 9154 | 345 / 13,6 | 4,0 / 0,157 | 100 / 1450 | 150 / 2176 |
| AC025 | 60 ÷ 150 / 3661 ÷ 9154 | 348 / 13,7 | 6,0 / 0,236 | 167 / 2422 | 250 / 3626 |
| AC053 | 60 ÷ 150 / 3661 ÷ 9154 | 348 / 13,7 | 7,1 / 0,280 | 200 / 2901 | 300 / 4351 |
| AD004 | 60 ÷ 180 / 3661÷ 10984 | 356 / 14,0 | 10,0 / 0,394 | 300 / 4351 | 450 / 6527 |
| Ø 393 ~ 406 mm | |||||
| AC030 | 80 ÷ 220 / 4882 ÷ 13425 | 406 / 16,0 | 5,5 / 0,217 | 63,7 / 924 | 98 / 1421 |
| AC051 | 80 ÷ 230 / 8442 ÷ 14035 | 393 / 15,5 | 6,9 / 0,272 | 167 / 2422 | 250 / 3626 |
| AC067 | 80 ÷ 150 / 4882 ÷ 9154 | 400 / 15,7 | 6,9 / 0,272 | 167 / 2422 | 250 / 3626 |
| AC083 | 80 ÷ 240 / 4882 ÷ 14645 | 405 / 15,9 | 6,9 / 0,272 | 167 / 2422 | 250 / 3626 |
| AC038 | 80 ÷ 180 / 4882 ÷ 10984 | 405 / 15,9 | 12,6 / 0,496 | 300 / 4351 | 450 / 6527 |
Gnee etkazib berish yuqori - yuqori bosim uchun issiq rulonli va sovuq po'latsiz po'latdan yasalgan truba va katta - Hajmi gazli gazsimon quvurlar. Biz po'lat quvurlar va boshqa quvurlarni yig'ish bo'yicha keng inventarizatsiya qilamiz, shunchaki bizga ehtiyojingizning o'lchami va miqdorini bizga ma'lum qilamiz va biz sizga to'g'ri keladigan materialni topishga yordam beramiz. Bugun bizga qo'ng'iroq qiling Jis G3429 chodirisiz po'latdan yasalgan sth12.