Sep 15, 2025 Xabar QOLDIRISH

Jis G3472 Avtomobil uchun uglerod po'lat naychasi

Jis G3472 Avtomobil tarkibiy maqsadlari uchun uglerod po'lat quvurlari

Linun - bu sifatli avtomobil tarkibiy strukturali naycha ishlab chiqaruvchisi, biz Rotorli Shibllar, Narxlar generallari va stabilizatorlardan olingan Axl yostiqlari va stabilizatorlardan olingan axl echimlari.

Jis g3472 Erv Tube Spetsifikatsiya:

Sint: Stam 290GB, Stam 390G, Stam 440G, Stam 470G
OD: 15.9-101.6mm
WT: 1.0-6.0MM
Uzunlik: 3000 - 9000 mm

Jis G3472 ERW Avtomobil tuzilishi po'lat naychasi Kimyoviy tarkibi jadvali:

Baho

Kimyoviy tarkibi %

C

Si

Mn

P

S

Stam 290GA

0,12 max.

0,35 max.

0.60 max.

0.035 max.

0.035 max.

Stam 290GB

Stam 340 g

0.20 max.

0,35 max.

0.60 max.

0.035 max.

0.035 max.

Stam 390g

0,25 max.

0,35 max.

0.30~0.90

0.035 max.

0.035 max.

Stam 440 g

Stam 440h

STAM 470G

Stam 470h

Stam 500g

0.30 max.

0,35 max.

0.30~1.00

0.035 max.

0.035 max.

Stam 500h

Stam 540h

Jis G3472 ERW Avtomobil tuzilishi po'lat naychasi mexanik xususiyatlari jadvali:

Baho

Belgi

Mustahkamlik chegarasi

(MPA)

Kuch berish kuchi
(MPA)

Cho'zish (1)%

Flash testi(2)

No.11-sonli test asari

Qo'ng'irlangan qo'ng'iroq qismining hajmi

(D: OD)

Bo'ylama yo'nalishi

G sinf

Stam 290GA

290 minut.

175 min.

40 daqiqa.

1.25 D

Stam 290GB

290 minut. 175 min. 35 min. 1.20 D

Stam 340 g

340 daqiqa.

195 daqiqa.

35 min.

1.20 D

Stam 390g

390 min.

235 daqiqa.

30 daqiqa.

1.20 D

Stam 440 g

440 daqiqa.

305 daqiqa.

25 minut.

1.15 D

STAM 470G

470 min. 325 daqiqa. 22 daqiqa. 1.15 D

Stam 500g

500 min.

355 min.

18 minut.

1.15 D
H sinf

Stam 440h

440 daqiqa.

355 min.

20 daqiqa.

1.15 D

Stam 470h

470 min.

410 daqiqa.

18 minut.

1.10 D

Stam 500h

500 min. 430 daqiqa. 16 minut. 1.10 D

Stam 540h

540 daqiqa.

480 min.

13 minut.

1.05 D

Jis G3472 Avtomobil mexanik naycha o'lchov jadvali:

Oq
(mm)
Vt (mm)
1.0 1.2 1.6 2.0 2.3 2.6 2.8 2.9 3.2 3.4 3.5 4.0 4.5 5.0 6.0
15.9 - 0.435 0.564 0.686 - - - - - - - - - - -
17.3 - - - 0.755 0.851 - - - - - - - - - -
19.1 0.446 0.530 0.690 0.843 0.953 - - - - - - - - - -
22.2 0.523 0.621 0.813 0.996 1.13 - - - - - - - - - -
25.4 - 0.716 0.939 1.15 - 1.50 - 1.61 - - - - - - -
28.6 - 0.811 1.07 1.31 - 1.67 - - - - - - - - -
31.8 0.760 0.906 1.19 1.47 1.67 - - - 2.26 - - - - - -
34.0 - - 1.28 - 1.80 - - - 2.43 - - 2.97 - - -
35.0 - 1.00 1.32 1.63 - - 2.22 2.32 - - - - - - -
38.1 0.915 1.09 1.44 1.78 2.03 - - - - - - - - - -
42.7 - 1.23 1.62 2.01 2.29 2.57 - - 3.12 - 3.38 - - 4.65 -
45.0 1.08 1.30 1.71 2.12 2.42 2.71 - 3.01 3.30 - - - 4.49 4.93 5.77
47.6 - 1.37 1.81 - 2.57 - - 3.20 - - - - - - -
48.6 - 1.40 1.85 2.30 2.63 - - 3.27 3.58 - - - 4.89 5.38 6.30
50.8 - 1.47 1.94 2.41 2.75 3.08 3.31 3.43 - 3.97 4.08 4.63 - - 6.63
54.0 - 1.56 2.07 - 2.93 3.29 3.54 3.65 - 4.24 4.36 4.95 - - -
57.0 - - 2.19 - 3.10 3.48 3.74 3.87 4.25 4.49 4.62 - - - -
60.5 - - 2.32 - 3.30 3.71 - 4.12 4.52 - - 5.59 - - -
63.5 - - 2.44 - - 3.90 - - - - - - - - -
65.0 - - 2.50 - - - - - 4.88 - 5.31 - - - -
68.9 - - 2.66 - 3.78 - - - - - - - - - -
70.0 - - 2.70 - - - - - 5.27 - 5.74 - - - -
75.0 - - 2.90 - 4.12 4.63 - 5.16 5.67 - - 7.03 - - -
80.0 - - 3.09 - - 4.96 - - 6.06 - - - - - -
82.6 - - - 3.98 4.55 - - - - - - - - - -
90.0 - - 3.49 - 4.97 5.59 - - 6.85 - - 8.51 - 10.5 12.4
94.0 - - 3.65 - - 5.86 - - 7.17 - - - - - -
101.6 - - - - - - - - - - - 9.66 - 11.9 14.1

 

info-400-266