Chirishsiz yoki payvandlangan

1. A234 WPB uchun harorat doirasi
** Baza materiallar ** -20 darajasi f ({1}} darajasi (-29 {343 daraja) (343 daraja) ga ARTM A 234.
** Payvandlangan to'qnashuvlar ** ** Payvandlash moslamalari ({1}}} darajasi ({1} qo'shimcha talablari) (800 daraja F) .} {{4} qo'shimcha talablar amalga oshirilgan bo'lsa, .

{{0} WPB vs . SA SA SA SA 420
| ** Xususiyat **|** SA 234 WPB **|** SA 420 WPL6 ** |
| ** Qo'llanma **|Uglerod po'lat ** Fitinglar **|Uglerod po'lat ** quvur ** |
| ** Harorat **|O'rtacha (-29} darajasiga qaraganda katta yoki teng)|** Kam harorat ** -46}} darajasiga ega) |
| ** tugmadan foydalanish **|Umumiy xizmat|Sub-nol / kriogenik xizmati |
| ** qattiqlik sinov **|Talab qilinmaydi (buyurtma qilingan bo'lsa)|** Majburiy ** Charpy V-Notch |

3. payvandlashda "WPB"
"WPB" ** {.} .} . {. {. {. {{. {{{}}}, E70xx-ni tanlang. elektrodlar yoki er70s-x simlari) .}

4. WPB VS . WPC
| ** Aspekt **|** WPB **|** WPC ** |
| ** Uglerod tarkibi **|0,30% dan kam yoki unga teng|0,25% dan kam yoki teng
| ** silikon **|0 . 10% min. Dokqalanish uchun|0,13% dan kam yoki teng
| ** Zenvaldagi kuch **|60-85 KSI (415-585 MPA)|** 70-95 KSI (485-655 MPA) |
| ** Ta'sir testi **|Kerakli emas|** talab qilinadi ** ({-20 ilmiy f / -29 ilmiy darajasi) |
| ** Umumiy foydalanish **|Umumiy quvur (asme b16.9)|Yuqori stress / evropalik xususiyatlar |

5. essiz yoki payvandlanganmi?
** A234 WPB fitts-terisiz yoki payvandlangan bo'lishi mumkin. va narx .

Muhim dasturlar uchun har doim ASTM standartlari, loyihaviy xususiyatlar va qo'llaniladigan kodlar (E . . . . . 3).