Galvanizli ichi bo'sh qismlar

Mahsulotlar tavsifi

Nomi: GI ichi bo'sh qism

Yuzaki: Galvanizli (odatda 40-60g/m2, mijoz talab qilishi mumkin)

OD: 10*15-100*150mm

WT:0.6-2,3 mm

Uzunlik: doimiy yoki tasodifiy, mijoz talabiga binoan

Shakl: to'rtburchaklar

Material: Q195 Q215 Q235

Savdo shartlari: FOB, C&F, CIF, EXW

To'lov shartlari: TT depoziti + BL nusxasi / LC yoki 100% LC ko'rinishida

Bo'shliq bo'limning spetsifikatsiyasi

Hajmi kg/m Std tegirmon uzunligi (m)
13x13x1,8 mm ** 0.57 6.5
15x15x1,8 mm ** 0.68 6.5
20x20x1,6 mm 0.87 6.5
25x25x1,6 mm 1.12 6.5
25x25x2.0 mm 1.36 6.5
25x25x2,5 mm 1.64 6.5
25x25x3.0 mm 1.89 6.5
30x30x1,6 mm 1.38 8.0
30x30x2,0 mm 1.68 8.0
30x30x2,5 mm 2.03 8.0
30x30x3,0 mm 2.36 8.0
35x35x1,6 mm 1.63 8.0
35x35x2.0mm 1.99 8.0
35x35x2,5 mm 2.42 8.0
40x40x1,6 mm 1.88 8.0
40x40x2,0 mm 2.31 8.0
40x40x2,5 mm 2.82 8.0
40x40x3,0 mm 3.30 8.0
40x40x4,0 mm 4.09 8.0
50x50x1,6 mm 2.38 8.0
50x50x2,0 mm 2.93 8.0
50x50x2,5 mm 3.60 8.0
50x50x3,0 mm 4.25 8.0
50x50x4,0 mm 5.35 8.0
50x50x5,0 mm 6.56 8.0
65x65x1,6 mm 3.31 8.0
65x65x2.0 mm 3.88 8.0
65x65x2,5 mm 4.78 8.0
65x65x3.0mm 5.66 8.0
65x65x4.0mm 7.23 8.0
75x75x2,5 mm 5.56 8.0
75x75x3.0 mm 6.60 8.0, 9.0, 12.0
75x75x4.0 mm 8.49 8.0, 9.0, 12.0
75x75x5.0mm 10.30 8.0
75x75x6.0mm 12.00 8.0
89x89x2.0mm 5.36 8.0, 12.0
100x100x3,0 mm 8.96 8.0, 12.0
100x100x4,0 mm 11.60 8.0, 12.0
100x100x5,0 mm 14.20 8.0
100x100x6,0 mm 16.70 8.0
125x125x4.0mm ** 14.80 8.0, 12.0
125x125x5.0mm ** 18.20 8.0, 12.0
125x125x6.0mm ** 21.40 8.0, 12.0
150x150x5,0 mm ** 22.10 8.0, 12.0
150x150x6,0mm ** 26.20 8.0, 12.0
200x200x5,0mm ** 29.90 8.0, 12.0
200x200x6,0mm ** 35.60 8.0, 12.0

To'rtburchaklar po'lat quvur

MILD STEEL HOLLOW SECTIONSERW Hollow Sections

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Bizning xizmatimiz

1. Kranlarni o'z vaqtida etkazib berishni ta'minlash uchun jarayonni qattiq nazorat qilish
2. Yuk tashish hujjatlari bilan yordam beramiz
3. Bizning katta muhandislarimiz o'rnatish bo'yicha ko'rsatmalar, ishga tushirish va o'qitish xizmatlarini taqdim etishlari mumkin.
4. Ingliz tilidagi foydalanuvchi qo'llanmalari, ehtiyot qismlar qo'llanmalari, mahsulot sertifikatlari va tegishli sertifikatlar yetkazib berish vaqtida taqdim etiladi.
5. O'rnatish va ishga tushirilgandan so'ng 12 oylik kafolat, insonga zarar etkazuvchi omil bundan mustasno.
6. Istalgan vaqtda texnik maslahatlarni taqdim eting va muhandislarni chet elda mashinaga xizmat ko'rsatishga majbur qiling.

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov