ASTM A182 zanglamaydigan po'lat quvur armatura

Zanglamas po'latdan yasalgan quvur armaturalari turli xil zanglamaydigan po'lat quvurlarni ulash ish qismlari uchun umumiy atamadir. Ular shakli, maqsadi, ulanish usuli va boshqalarga ko'ra turli toifalarga bo'linishi mumkin. U oson o'rnatish, yuqori ishlash va chidamlilik xususiyatlariga ega va turli quvurlarni qurish va o'rnatishda keng qo'llaniladi.
So'rov yuborish
Hozir chat
Mahsulotni tanishtirish

A182 yuqori haroratli ob'ekt klapanlari va gardish quvurlari armaturalari uchun Amerika standartidagi zanglamaydigan po'latdan yasalgan zarblarga tegishli. A182 zanglamaydigan po'lat, shuningdek, ultra past karbonli zanglamaydigan po'lat sifatida ham tanilgan, ko'p qirrali zanglamaydigan po'latdan yasalgan material bo'lib, bosimli idishlar, uskunalar va yaxshi keng qamrovli xususiyatlarni (korroziyaga chidamlilik va shakllanish) talab qiladigan qismlarni ishlab chiqarish uchun keng qo'llaniladi.

Savdo nomi

Baho

UNS % 23

Soxta armatura

304

F304

S30400

A182 % 2f SA182

304L

F304L

S30403

A182 % 2f SA182

304H

F304H

S30409

A182 % 2f SA182

316

F316

S31600

A182 % 2f SA182

316L

F316L

S31603

A182 % 2f SA182

316H

F316H

S31609

A182 % 2f SA182

321

F321

S32100

A182 % 2f SA182

321H

F321H

S32109

A182 % 2f SA182

347

F347

S34700

A182 % 2f SA182

347H

F347H

S34709

A182 % 2f SA182

317L

F317L

S31703

A182 % 2f SA182

Kimyoviy xossalari %

Baho C Mn P S Si Ni Cr Moʻy
ASTM A182 F304 0.08 2 0.045 0.03 1 8.0-11.0 18.0-20.0
ASTM A182 F304H 0.04-0.10 2 0.045 0.03 1 8.0-11.0 18.0-20.0
ASTM A182 F304L 0.03 2 0.045 0.03 1 8.0-13.0 18.0-20.0
ASTM A182 F304N 0.08 2 0.045 0.03 1 8.0-10.5 18.0-20.0
ASTM A182 F304LN 0.03 2 0.045 0.03 1 8.0-10.5 18.0-20.0
ASTM A182 F309H 0.04-0.10 2 0.045 0.03 1 12.0-15.0 22.0-24.0
ASTM A182 F310 0.25 2 0.045 0.03 1 19.0-22.0 24.0-26.0
ASTM A182 F310H 0.04-0.10 2 0.045 0.03 1 19.0-22.0 24.0-26.0
ASTM A182 F310MoLN 0.03 2 0.03 0.015 0.4 21.0-23.0 24.0-26.0 2.0-3.0
ASTM A182 F316 0.08 2 0.045 0.03 1 10.0-14.0 16.0-18.0 2.0-3.0
ASTM A182 F316H 0.04-0.10 2 0.045 0.03 1 10.0-14.0 16.0-18.0 2.0-3.0
ASTM A182 F316L 0.03 2 0.045 0.03 1 10.0-15.0 16.0-18.0 2.0-3.0
ASTM A182 F316N 0.08 2 0.045 0.03 1 11.0-14.0 16.0-18.0 2.0-3.0
ASTM A182 F316LN 0.03 2 0.045 0.03 1 11.0-14.0 16.0-18.0 2.0-3.0
ASTM A182 F316Ti 0.08 2 0.045 0.03 1 10.0-14.0 16.0-18.0 2.0-3.0
ASTM A182 F317 0.08 2 0.045 0.03 1 11.0-15.0 18.0-20.0 3.0-4.0
ASTM A182 F317L 0.03 2 0.045 0.03 1 11.0-15.0 18.0-20.0 3.0-4.0
ASTM A182 F321 0.08 2 0.045 0.03 1 9.0-12.0 17.0-19.0
ASTM A182 F321H 0.04-0.10 2 0.045 0.03 1 9.0-12.0 17.0-19.0
ASTM A182 F347 0.08 2 0.045 0.03 1 9.0-13.0 17.0-20.0
ASTM A182 F347H 0.04-0.10 2 0.045 0.03 1 9.0-13.0 17.0-20.0
ASTM A182 F348 0.08 2 0.045 0.03 1 9.0-13.0 17.0-20.0
ASTM A182 F348H 0.04-0.10 2 0.045 0.03 1 9.0-13.0 17.0-20.0

Mexanik xususiyatlar

Baho Kuchlanish kuchi (Mpa) Chiqish nuqtasi (Mpa) Uzayish (%) Kamaytirish (%)
ASTM A182 F304 515 205 30 50
ASTM A182 F304L 485 170 30 50
ASTM A182 F316 515 205 30 50
ASTM A182 F316L 485 170 30 50
ASTM A182 F321 515 205 30 50

Zanglamaydigan po'latdan yasalgan armatura

SS Pipe FittingSS Pipe Elbows

Issiq teglar: astm a182 zanglamaydigan po'lat quvur armatura, Xitoy astm a182 zanglamaydigan po'lat quvur armatura ishlab chiqaruvchilari, etkazib beruvchilari

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov