Katta diametrli karbonli po'latdan yasalgan qopqoq
Bosim idishining muhrlanishini ta'minlash uchun bosh muhim komponent hisoblanadi. Tsilindrga payvandlangan va uni qismlarga ajratib bo'lmaydigan har qanday narsa bosh deb ataladi;
Material:Karbonli po'lat ASME / ASTM SA / A234 WPB, DIN 1.0405
Hajmi:ANSI B16.9, ANSI B16.28, JIS B2312, JIS B2313
Qalinligi:Jadval 5S, 10S, 20S, S10, S20, S30, STD, 40S, S40, S60, XS, 80S, S80, S100, S120, S140, S160, XXS va boshqalar.
Quvur qopqog'ining o'lchami: 1/2″~48″
Q235B Qopqoqning kimyoviy xossalari
|
Kimyoviy xossalari % |
|||||||||
|
A sinf |
|||||||||
|
C |
Mn |
P |
S |
Si |
Cr |
Oʻt |
Moʻy |
Ni |
V |
|
0.25 |
0.27-0.93 |
0.035 |
0.035 |
0.1 |
0.4 |
0.4 |
0.15 |
0.4 |
0.08 |
|
B sinf |
|||||||||
|
C |
Mn |
P |
S |
Si |
Cr |
Oʻt |
Moʻy |
Ni |
V |
|
0.3 |
0.29-1.06 |
0.035 |
0.035 |
0.1 |
0.4 |
0.4 |
0.15 |
0.4 |
0.08 |
|
C darajasi |
|||||||||
|
C |
Mn |
P |
S |
Si |
Cr |
Oʻt |
Moʻy |
Ni |
V |
|
0.35 |
0.29-1.06 |
0.035 |
0.035 |
0.1 |
0.4 |
0.4 |
0.15 |
0.4 |
0.08 |
Q235B quvur qopqog'ining mexanik xususiyatlari
|
Mexanik xususiyatlar |
|||
|
|
A sinf |
B sinf |
C darajasi |
|
Mustahkamlik chegarasi |
330 |
415 |
485 |
|
Hosildorlik kuchi |
205 |
240 |
275 |
Karbonli po'lat quvur qopqog'i OD o'lchami jadvali
| Tashqi diametri | Yuqori o'lcham | Devor qalinligi "E" ga mos keladi | ||
| DN | NPS | E | E1 | E |
| 15 | 1/2 | 25 | 25 | 3.73 |
| 20 | 3/4 | 25 | 25 | 3.91 |
| 25 | 1 | 38 | 38 | 4.55 |
| 32 | 1 1/4 | 38 | 38 | 4.85 |
| 40 | 1 1/2 | 38 | 38 | 5.08 |
| 50 | 2 | 38 | 44 | 5.54 |
| 65 | 2 1/2 | 38 | 51 | 7.01 |
| 80 | 3 | 51 | 64 | 7.62 |
| 90 | 3 1/2 | 64 | 76 | 8.08 |
| 100 | 4 | 64 | 76 | 8.56 |
| 125 | 5 | 76 | 89 | 9.53 |
| 150 | 6 | 89 | 102 | 10.97 |
| 200 | 8 | 102 | 127 | 12.7 |
| 250 | 10 | 127 | 152 | 12.7 |
| 300 | 12 | 152 | 178 | 12.7 |
| 350 | 14 | 165 | 191 | 12.7 |
| 400 | 16 | 178 | 203 | 12.7 |
| 450 | 18 | 203 | 229 | 12.7 |
| 500 | 20 | 229 | 254 | 12.7 |
| 550 | 22 | 254 | 254 | 12.7 |
| 600 | 24 | 267 | 305 | 12.7 |
| 650 | 26 | 267 | ||
| 700 | 28 | 267 | ||
| 750 | 30 | 267 | ||
| 800 | 32 | 267 | ||
| 850 | 34 | 267 | ||
| 900 | 36 | 267 | ||
| 950 | 38 | 305 | ||
| 1000 | 40 | 305 | ||
| 1050 | 42 | 305 | ||
| 1100 | 44 | 343 | ||
| 1150 | 46 | 343 | ||
| 1200 | 48 | 343 | ||
Uglerod quvurining oxiri qopqog'i


Issiq teglar: katta diametrli karbonli po'lat qopqoq, Xitoyning katta diametrli karbonli po'lat qopqoq ishlab chiqaruvchilari, etkazib beruvchilari
Oldingi
Payvandlangan gardishKeyingi2
Oxirgi qopqoqSizga ham yoqishi mumkin
So'rov yuborish