A213 T5 T9 T11 payvandlangan quvur
A213 T5 T9 T11 payvandlangan quvur yetkazib beruvchi-GNEE
ASTM A213 (ASME SA213) quvurlari yuqori haroratli uskunalarda, ayniqsa, qozonlarda va super isitgichlarda keng qo'llanilgan. Quvurlar qotishma po'latdan va zanglamaydigan po'latdan tayyorlanishi mumkin va issiq haddeleme yoki sovuq chizish bilan muammosiz ishlab chiqariladi. Umumiy navlarga T5, T9, T11, T12, T21, T22, T91 va zanglamaydigan po'latdan TP304 yoki TP316 navlari kiradi.
Asosiy navlar: ASTM A213 T5, T5b, T9, T11, T91 va T22
O'lcham oralig'i:
NPS 1/4'' dan NPS 24''gacha
Devor qalinligi - 40 dan 160 gacha bo'lgan jadvallar, STD, XS, XXS.
Rejadan tashqari og'ir devor quvurlari qalinligi 4 dyuymgacha mavjud.
A213 T5 T9 T11 payvandlangan po'lat quvur o'lchamlari
|
NPS, dyuym |
Tashqi diametri (mm) |
Devor qalinligi (mm) |
Maks. Uzunlik (M) |
|
1/8 |
10,3 |
1,24; 1,73; 2,40 |
12 |
|
1/4 |
13,7 |
1,65; 2,24; 3,02 |
|
|
3/8 |
17,1 |
1,65; 2,31; 3,20 |
|
|
1/2 |
21,3 |
1,65; 2,11; 2,77; 3,73 |
|
|
3/4 |
26,7 |
1,65; 2,11; 2,87; 3,91 |
|
|
1 |
33,4 |
1,65; 2,77; 3,38; 4,55 |
10 |
|
1 1/4 |
42,4 |
1,65; 2,77; 3,56; 4,85 |
|
|
1 1/2 |
48,3 |
2,77; 3,68; 5,08 |
|
|
2 |
60,3 |
3,91; 5,54 |
7 |
|
2 1/2 |
73,0 |
5,16; 7,01 |
Zanglamaydigan po'latdan payvandlangan quvur mexanik xususiyatlari
|
Baho |
Mustahkamlik chegarasi |
Chiqish nuqtasi (Mpa) |
Uzayish (%) |
Ta'sir (J) |
Qattiqlik |
|
A213 T2/SA213 T2 |
415 dan katta yoki unga teng |
205 |
|
" |
85HRB |
|
A213 T11/SA213 T11 |
415 dan katta yoki unga teng |
205 |
|
" |
85HRB |
|
A213 T22/SA213 T22 |
415 dan katta yoki unga teng |
205 |
|
" |
85HRB |
|
A213 T23/SA213 T23 |
510 dan katta yoki teng |
400 |
20 |
" |
97HRB |
|
A213 T24/SA213 T24 |
585 dan katta yoki unga teng |
415 |
20 |
" |
25HRB |
|
A213 T91/SA213 T91 |
585 dan katta yoki unga teng |
415 |
20 |
" |
25HRB |
|
A213 T911/SA213 T911 |
620 dan katta yoki unga teng |
440 |
20 |
" |
25HRB |
|
A213 T22/SA213 T92 |
620 dan katta yoki unga teng |
440 |
20 |
" |
25HRB |
|
A213 T122/SA213 T122 |
620 dan katta yoki unga teng |
400 |
20 |
|
25HRB |
|
TP304H |
515 dan katta yoki unga teng |
205 |
35 |
|
90HRB |
|
TP316H |
515 dan katta yoki unga teng |
205 |
35 |
|
90HRB |
|
TP321H |
515 dan katta yoki unga teng |
205 |
35 |
|
90HRB |
|
TP347H |
515 dan katta yoki unga teng |
205 |
35 |
|
90HRB |
|
S30432 |
590 dan katta yoki unga teng |
235 |
35 |
|
95HRB |
|
TP310HCbN |
655 dan katta yoki unga teng |
295 |
30 |
|
100 HRB |
A213 T5 T9 T11 ERW quvur detali


Issiq teglar: a213 t5 t9 t11 payvandlangan quvur, Xitoy a213 t5 t9 t11 payvandlangan quvur ishlab chiqaruvchilari, etkazib beruvchilari
Keyingi2
2507 zanglamaydigan po'lat quvurSizga ham yoqishi mumkin
So'rov yuborish