Katta diametrli zanglamaydigan po'lat quvur
Devor qalinligi: SCH 5, 5S, 10, 10S, 20, 30, 40, 40S, 60, 80, 80S, 100, 120, 140, 160, STD, XS va XXS, 1,24 mm dan 25,4 mm gacha.
Uzunlikka kesish: tasodifiy uzunlik taklif qilinishi mumkin, maksimal uzunligi 20 metr va sobit quvur uzunligi 6 metr bo'lishi mumkin.
Katta diametrli zanglamaydigan quvur tavsifi
Tashqi diametri 200 mm (8 dyuym) dan katta bo'lgan zanglamaydigan po'lat quvurlar odatda tabiiy gaz, neft va boshqalarni tashish uchun ishlatiladigan katta diametrli zanglamaydigan po'lat quvurlarga aylanadi.
GNEE Group professional katta diametrli zanglamaydigan po'lat quvur ishlab chiqaruvchisi sifatida 3 ta katta diametrli zanglamaydigan po'lat quvur ishlab chiqarish liniyasiga va 2 ta kichik diametrli zanglamaydigan po'lat quvur ishlab chiqarish liniyasiga ega. Biz A312, A358, A269, A789 va boshqalar kabi zanglamas po'latdan yasalgan quvurlar standartlarini etkazib bera olamiz. po'lat dumaloq quvur, zanglamaydigan po'latdan yasalgan to'rtburchaklar quvur va boshqalar Biz boshqa etkazib beruvchilarga qaraganda pastroq narxni taklif qilishimiz mumkin, agar siz qiziqsangiz, kotirovka uchun biz bilan bog'lanishingiz mumkin.
Katta diametrli zanglamaydigan quvurlar spetsifikatsiyasi
| Spetsifikatsiya | ASTM A312, ASTM A778, ASTM A358, ASTM A999 |
| Standart | ASTM, ASME va API |
| Hajmi | EFW - 8" NB TO 110" NB (nominal teshik hajmi) |
| Turlari | Elektr-fusion-payvandlangan, choksiz, polyak va boshqalar. |
| Uzunlik | 01 metrdan 12,5 metrgacha, bitta tasodifiy uzunlik, ikki marta tasodifiy uzunlik va moslashtirilgan o'lcham. |
| Tashqi diametri | 6.00 mm OD 914,4 mm gacha, oʻlchami 24” NB gacha |
| Devor qalinligi | (3 mm dan 100 mm gacha qalinligi) SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Oxiri | To‘g‘ri uchi, qirrali uchi, pog‘onali |
| To'lov muddati | T/T, L/C, va hokazo. |
Zanglamaydigan po'lat quvurlar navlari
| Baho | Uglerod | Kremniy | Marganets | Chromium | Nikel | Molibden | Oltingugurt | Fosforli |
|---|---|---|---|---|---|---|---|---|
| TP304 | 0,08 | 1,0 | 2.00 | 18.0 – 20.0 | 8.0 – 11.0 | – | 0,03 | 0,045 |
| TP304L | 0,035 | 1,0 | 2.00 | 18.0 – 20.0 | 8.0 – 13.0 | – | 0,03 | 0,045 |
| TP316 | 0,08 | 1,0 | 2.00 | 16.0 – 18.0 | 10.0 – 14.0 | 2.00 – 3.00 | 0,03 | 0,045 |
| TP316L | 0,035 | 1,0 | 2.00 | 16.0 – 18.0 | 10.0 – 15.0 | 2.00 – 3.00 | 0,03 | 0,045 |
| TP321 | 0,08 | 1,0 | 2.00 | 17.0 – 19.0 | 9.0 – 12.0 | – | 0,03 | 0,045 |
Sanoat quvurlari uchun katta diametrli zanglamaydigan po'lat quvur
| Katta diametrli o'lchagichlar uchun spetsifikatsiya (Xususiyatlar va o'lchamlar faqat ASME B36.19M uchun) | |||||
| DN | Tashqi diametri | Nominal devor qalinligi | |||
| SCH 5S | SCH 10S | SCH 40S | |||
| DN | NPS | mm | mm | mm | mm |
| 350 | 14" | 355.6 | 3.96 | 4.78 | 9.53 |
| 400 | 16" | 406.4 | 4.19 | 4.78 | 9.53 |
| 450 | 18" | 457 | 4.19 | 4.78 | 9.53 |
| 500 | 20" | 508 | 4.78 | 5.54 | 9.53 |
| 550 | 22" | 559 | 4.78 | 5.54 | - |
| 600 | 24" | 610 | 5.54 | 6.35 | 9.53 |
| 750 | 30" | 762 | 6.35 | 7.92 | - |
Katta zanglamaydigan po'lat quvurlar uchun mexanik xususiyat
| Baho | Mexanik xossalar | ||||
| Mustahkamlik chegarasi | Kuchli kuch | Cho'zilish | Qattiqlik | ||
| KSi(MPa) | KSi(MPa) | % | HRB | ||
| ASTM | TP304 | 75 (515) dan kichik yoki unga teng | 30 dan kichik yoki teng (205) | 35 dan kam yoki teng | 90 dan kam yoki teng |
| TP304L | 70 dan kam yoki teng (483) | 25 dan kichik yoki teng (170) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| TP316 | 75 (515) dan kichik yoki unga teng | 30 dan kichik yoki teng (205) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| TP316L | 70 dan kam yoki teng (483) | 25 dan kichik yoki teng (170) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| JIS | SUS304 | 75 (520) dan kichik yoki unga teng | 30 dan kichik yoki teng (206) | 35 dan kam yoki teng | 90 dan kam yoki teng |
| SUS304L | 70 dan kichik yoki teng (481) | 25 dan kichik yoki teng (177) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| SUS316 | 75 (520) dan kichik yoki unga teng | 30 dan kichik yoki teng (206) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| SUS316L | 70 dan kichik yoki teng (481) | 25 dan kichik yoki teng (177) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| GB | 0Crl8Ni9 | 75 (520) dan kichik yoki unga teng | 30 dan kichik yoki teng (210) | 35 dan kam yoki teng | 90 dan kam yoki teng |
| {0}}Crl9Nil0 | 70 dan kam yoki teng (480) | 25 dan kichik yoki teng (180) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| 0Crl7Nil2Mo2 | 75 (520) dan kichik yoki unga teng | 30 dan kichik yoki teng (210) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| 00Crl7Nil4Mo2 | 70 dan kam yoki teng (480) | 25 dan kichik yoki teng (180) | 35 dan kam yoki teng | 90 dan kam yoki teng | |
| UZ10217-7 | 1.4301 | (500-700) | Kichik yoki teng (195) | >40b | 90 dan kam yoki teng |
| 1.4307 | (470-670) | Kichik yoki teng (180) | >40b | 90 dan kam yoki teng | |
| 1.4401 | (510-710) | Kichik yoki teng (205) | >40b | 90 dan kam yoki teng | |
| 1.4404 | (490-690) | Kichik yoki teng (190) | >40b | 90 dan kam yoki teng | |
Katta diametrli po'lat quvur


GNEE ta'minoti zanglamaydigan po'lat quvur turlari
| Zanglamaydigan po'latdan yasalgan egzoz trubkasi | Zanglamaydigan po'latdan yasalgan dumaloq quvur |
| Jilolangan zanglamaydigan quvur | Oval po'lat quvur |
| Zanglamaydigan choksiz quvur | Yupqa devorli zanglamaydigan quvurlar |
| Zanglamaydigan po'latdan payvandlangan quvur | Yuqori bosimli zanglamaydigan po'lat quvur |
| Zanglamaydigan po'latdan yasalgan kvadrat quvur | ERW SS trubkasi |
Nima uchun GNEE SS po'lat quvurini tanlaysiz?
- GNEE Group katta diametrli zanglamaydigan po'lat quvurlarni ishlab chiqarish va yetkazib berish bo'yicha 16 yillik tajribaga ega.
- GNEE tomonidan ishlab chiqarilgan zanglamaydigan po'lat quvurlar Metline tomonidan ishlab chiqarilganlarga qaraganda ancha tejamkor.
- Har yili biz dunyo bo'ylab 50 million tonnadan ortiq zanglamaydigan po'lat quvurlarni etkazib beramiz.
- Biz mahsulotlar, logistika va qadoqlash kabi barcha ehtiyojlaringizni qondirish uchun bir martalik xizmatni taklif qilamiz.
- Biz SGS, ISO, Idoralar, zavod tekshiruvi hisobotlari va uchinchi tomon tekshiruv hisobotlarini taqdim etamiz.
- Zanglamaydigan po'lat quvurlarni yoki boshqa po'lat quvurlarni moslashtirish qo'llab-quvvatlanadi.

Issiq teglar: katta diametrli zanglamaydigan po'lat quvur, Xitoyning katta diametrli zanglamaydigan po'lat quvur ishlab chiqaruvchilari, etkazib beruvchilari
Sizga ham yoqishi mumkin
So'rov yuborish