API 5L darajasidagi X42 ERW liniyasi quvuri
Turi: ERW/ Payvandlangan
To'lov shartlari: T / T, L / C
Yetkazib berish muddati: Depozitni olgandan keyin 7-25 kun.
API 5L X42 ERW quvur tavsifi
API 5L X42 welded pipe: API stands for the American Petroleum Institute, with "X" denoting the first letter of "pipeline" in English, capitalized; "42" indicates a minimum yield strength of >420 MPa. X42 quvur liniyasi trubkasi X42 po'latdan yasalgan quvur liniyasi bo'lib, tekis uchlari, tishli uchlari va rozetka uchlari mavjud. U payvandlash, ulash, rozetkaga ulanish va boshqalar orqali ulanadi API 5L X42 payvandlangan quvur odatda neft va tabiiy gaz uzatish quvurlarini qurishda qo'llaniladi.
PSL-1 bahosi:
Quvur quvurlari X42/L290 poʻlat markasi: C 0.28% dan kam yoki teng, Mn 1.30% dan kam yoki teng, P {{ dan kam yoki teng 12}}.030%, S 0 dan kichik yoki teng.030%, Nb+V+Ti 0,06% dan kam yoki teng, Cu 0,50% dan kam yoki unga teng, Ni 0,50% dan kam yoki teng, Cr 0,50% dan kam yoki teng, Mo 0,15% dan kam yoki teng.
PSL-2 bahosi:
Quvur trubkasi L290N/X42N po'lat markasi: C 0.24% dan kam yoki teng, Mn 1,20% dan kam yoki teng, P { dan kam yoki teng {10}.025%, S 0 dan kichik yoki teng.015%, Nb {{2{{22 dan kam yoki teng }}}}.05%, V 0,06% dan kam yoki unga teng, Ti 0,04% dan kam yoki teng, Cu 0,50% dan kam yoki teng, Ni 0,30% dan kam yoki teng, Cr 0,30% dan kam yoki unga teng, Mo 0,15% dan kam yoki teng, B 0,004% dan kam yoki teng.
Quvur quvuri L290M/X42M markasi: C dan kam yoki unga teng 0,22%, Mn 1,30% dan kam yoki teng, P {{ dan kam yoki teng 10}.025%, S 0 dan kichik yoki teng.015%, Nb {{2{{22} dan kichik yoki teng }}}.05%, V 0,05% dan kam yoki unga teng, Ti 0,04% dan kam yoki teng, Cu 0,50% dan kam yoki teng, Ni 0,30% dan kam yoki teng, Cr Kam dan yoki 0,30% ga teng, Mo 0,15% dan kam yoki teng, B 0,004% dan kam yoki teng.
API 5L standarti X42/L290 materialning kuchlanish sinovi talablari:
PSL-1 Darajasi: Chiqish kuchi 290MPa dan katta yoki unga teng, tortishish kuchi 415MPa dan katta yoki unga teng.
PSL{0}} Darajasi: Chiqish kuchi 290MPa~495MPa, tortishish kuchi: 415MPa~655MPa, Chiqish nisbati 0,93 dan kam yoki unga teng.
API 5L X42 ERW trubkasi spetsifikatsiyasi
| Baho | X42 / L290 (N, M, Q, R) X42 PSL1: 1.0483 X42 PSL2: 1.0484 |
| Standart | API 5L |
| O.D. | 16" dan 54" gacha |
| Quvur oxiri |
Buttweld, vibrator silliqlash, qirrali uchi (BE), kesilgan yivlar, tekis uchi (PE), vidalangan, gardishli uchlari, yivli, rozetka, paxsa, tishli uchlari (erkak va urg'ochi), ipni kesish |
| Devor qalinligi | SCH160, SCH40, SCH-XXS, SCH-XS, SCH-STD, SCH80, |
API 5L X42 ERW po'lat quvur


Issiq teglar: api 5l gradusli x42 erw trubkasi, Xitoy api 5l gradusli x42 erw quvur ishlab chiqaruvchilari, etkazib beruvchilari