ERW Po'lat quvur API 5CT
API 5CT da xom ashyo to'rt guruhga bo'lingan. 1-guruh - H, J, K, N, 2-guruh - C, L, M, T, 3-guruh - P, 4-guruh - Q. Ular orasida J55, K55 va N kabi farqlar mavjud{{7} }N80-O. Asosan, ular moddiy xususiyatlarning raqamli diapazoni bo'yicha (po'lat navi, prokat, issiqlik bilan ishlov berish va nihoyat ishlash) bo'linadi. Har bir guruhdagi po'lat navlarini tasniflashga kelsak, ular ham xususiyatlariga ko'ra bo'linadi.
API 5CT ERW quvurlari spetsifikatsiyasi
|
Turi |
Korpus va quvurlar uchun API ERW po'lat quvur |
|
|
Ijroiya standarti |
API 5L |
|
|
Materiallar |
PSL1-L245B/L290X42/L320X46/L360X52/L390X56/L415X60/L450X65/L485X70 PSL% 7b{0}}L245/L290/L320/L360/L390/L415%2 ff450/L485 X42/X46/X52/X52/X56/X60/X65/X70/X80 |
|
|
Hajmi |
Tashqi diametri |
Uzluksiz:17-914mm 3/8"-36" |
|
Devor qalinligi |
2-60mm SCH10 SCH20 SCH30 STD SCH40 SCH60 XS SCH80 SCH100 SCH120 SCH140 SCH160 XXS |
|
|
Uzunlik |
Yagona tasodifiy uzunlik / Ikki tasodifiy uzunlik 5m-14m,5,8m,6m,10m-12m,12m yoki mijozning haqiqiy talabiga binoan |
|
|
Tugaydi |
To'g'ri uchi / qiyshiq, ikkala uchida plastik qopqoqlar bilan himoyalangan, kesilgan, yivli, tishli va muftali va boshqalar. |
|
|
Yuzaki ishlov berish |
Yalang'och, bo'yash qora, laklangan, galvanizli, korroziyaga qarshi 3PE PP/EP/FBE qoplamasi |
|
|
Texnik usullar |
Issiq haddelenmiş / Sovuq chizilgan / Issiq kengaytirilgan |
|
|
Sinov usullari |
Bosim sinovi, nuqsonlarni aniqlash, girdob oqimi sinovi, gidrostatik sinov yoki ultratovush tekshiruvi, shuningdek, kimyoviy va fizik mulkni tekshirish |
|
|
Qadoqlash |
Kuchli po'lat chiziqlar bilan to'plamlardagi kichik quvurlar, bo'shashgan katta bo'laklar Shuningdek, mijozning talabiga binoan |
|
|
Ilova |
Neft gazi va suvni tashish |
|
|
Sertifikatlar |
API ISO |
|
|
MOQ |
10 tonna |
|
|
Ta'minot quvvati |
5000 T/M |
|
|
Yetkazib berish vaqti |
Odatda avans toʻlovi olinganidan keyin 25-35 kun ichida |
|
API 5CT korpus trubasining kimyoviy tarkibi
| Standart | Baho | Kimyoviy tarkibi (%) | |||||||||
| API SPEC 5CT | J55 | C | Si | Mn | P | S | Cr | Ni | Oʻt | Moʻy | V |
| K55 | 0.34-0.39 | 0.20-0.35 | 1.25-1.50 | 0.020 dan kichik yoki unga teng | 0 dan kichik yoki unga teng.015 | 0 dan kichik yoki unga teng.15 | 0 dan kichik yoki unga teng.20 | 0 dan kichik yoki unga teng.20 | / | / | |
| N80 | 0.34-0.38 | 0.20-0.35 | 1.45-1.70 | 0.020 dan kichik yoki unga teng | 0 dan kichik yoki unga teng.015 | 0 dan kichik yoki unga teng.15 | / | / | / | 0.11-0.16 | |
| L80 | 0.15-0.22 | 1 dan kichik yoki unga teng.00 | 0.25-1.00 | 0.020 dan kichik yoki unga teng | 0.010 dan kichik yoki unga teng | 12.0-14.0 | 0 dan kichik yoki unga teng.20 | 0 dan kichik yoki unga teng.20 | / | / | |
| P110 | 0.26-0.395 | 0.17-0.37 | 0.40-0.70 | 0.020 dan kichik yoki unga teng | 0.010 dan kichik yoki unga teng | 0.80-1.10 | 0 dan kichik yoki unga teng.20 | 0 dan kichik yoki unga teng.20 | 0.15-0.25 | 0 dan kichik yoki unga teng.08 | |
API 5CT quvurining mexanik xususiyatlari
| Baho | Turi | Yuk ostida umumiy cho'zilish (%) | Oqim kuchi (min) | Oqim kuchi (maksimal) | Kuchlanish kuchi min Mpa | Maksimal qattiqlik (HRC) | Qattiqlik Maks (HBW) |
| J55 | - | 0.5 | 379 | 552 | 517 | - | - |
| K55 | - | 0.5 | 379 | 552 | 655 | - | - |
| N80 | 1 | 0.5 | 552 | 758 | 689 | - | - |
| N80 | Q | 0.5 | 552 | 758 | 689 | - | - |
| L80 | 1 | 0.5 | 552 | 655 | 655 | 23 | 241 |
| L80 | 9Cr | 0.5 | 552 | 655 | 655 | 23 | 241 |
| L80 | 13Cr | 0.5 | 552 | 655 | 655 | 23 | 241 |
| C90 | - | 0.5 | 621 | 724 | 689 | 25.4 | 255 |
| C95 | - | 0.5 | 655 | 758 | 724 | - | - |
| T95 | - | 0.5 | 655 | 758 | 724 | 25.4 | 255 |
| P110 | - | 0.6 | 758 | 965 | 862 | - | - |
| Q125 | Hammasi | 0.65 | 862 | 1034 | 931 | - | - |
API 5CT ERW quvuri