Apr 03, 2024 Xabar QOLDIRISH

ASTM A269 zanglamaydigan po'lat quvur

Mahsulotlar tavsifi

ASTM A269 choksiz va payvandlangan quvurlarning texnik xususiyatlari

Hajmi 1/8 "OD dan 6" OD gacha
Qalinligi ANSI B36.19/36.10 ga muvofiq 1 mm dan 20 mm gacha, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S
Uzunlik 6 metrgacha, maxsus kesilgan uzunliklar
Turi Umumiy xizmat ko'rsatish uchun choksiz va payvandlangan ostenitik zanglamaydigan po'lat quvurlar
Baholar SS 304, SS 201, SS 304L, SS 316L, SS 202, SS 321H, SS 347

ASTM A269 TP304 TP304L TP316 TP316L zanglamaydigan po'lat quvurining kimyoviy tarkibi

Baho UNS
Dizayn
Tarkibi, %
C Mn P S Si Cr Ni Mo Ti Nb N Cu Ce B Al
TP304 S30400 0.08 2 0.045 0.03 1 18.0–20 8.0–11 . . . . . . . . . . . . . . . . . .    
TP304L S30403 0.035 2 0.045 0.03 1 18.0–20 8.0–13 . . . . . . . . . . . . . . . . . .    
TP304LN S30453 0.035 2 0.045 0.03 1 18.0–20 8.0–11 . . . . . . . . . 0.10-0.16 . . . . . .    
TP316 S31600 0.08 2 0.045 0.03 1 16.0–18 10.0–14 2.00–3 . . . . . . . . . . . . . . .    
TP316L S31603 0.035 2 0.045 0.03 1 16.0–18 10.0–15 2.00–3 . . . . . . . . . . . . . . .    
TP316LN S31653 0.035 2 0.045 0.03 1 16.0–18 10.0–13 . . . . . . . . . 0.10-0.16 . . . . . .    
TP317 S31700 0.08 2 0.045 0.03 1 18.0–20 11.0–15 3.0–4 . . . . . . . . . . . . . . .    
TP321 S32100 0.08 2 0.045 0.03 1 17.0–19 9.0–12 . . . . . . . . . . . . . . . . . .    
TP347 S34700 0.08 2 0.045 0.03 1 17.0–19 9.0–13 . . . . . . . . . . . . . . . . . .    
TP348 S34800 0.08 2 0.045 0.03 1 17.0–19 9.0–12.0 . . . 0.10 . . . . . . . . . . . .   C:

0.20

maks

. . . S31254 0.020 2 0.045 0.035 1 19.5–20.5 17.5-18.5 6.0-6.5 . . . . . . 0.18-0.22 0.50-1.50 . . .   . . .

ASTM A269 zanglamaydigan quvurlar

welded stainless steel tubingSeamless Stainless-Steel Tubes

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 