Apr 11, 2024 Xabar QOLDIRISH

A269 zanglamaydigan po'latdan payvandlangan quvur

Mahsulotlar tavsifi
Baholar 202, 304, 304L, 304H, 304LN, 316LN, 309S, 310S, 316, 316L, 316H, 316Ti, 317L, 321, 321H, 347, 345, ALL, 345 MO, 6MOLY, UNS S31254 va boshqalar.
Turi Choksiz / payvandlangan / sovuq chizilgan / ERW / EFW / issiq tugatish / sovuq tugatish
Tashqi diametri o'lchami CHIKSIZ - 6 MM OD TO 114,3 MM OD
Payvandlangan / ERW- 10 MM TO 114,3 MM OD
Devor qalinligi 0.8 MM TO 4 MM DEVOR QALINLIGI
Uzunlik 01 metrdan 12,5 metrgacha, bitta tasodifiy uzunlik, ikki marta tasodifiy uzunlik va moslashtirilgan o'lcham.
Tugaydi Oddiy uchlari, qiyshiq uchlari
Quvurlarni qoplash Mexanik jilo, elektropolish, saten qoplamasi, passivlangan
Sinov Mahsulotni tahlil qilish, rentgenografik tekshirish, ko'ndalang taranglik, tekislash, silliqlash, barqarorlashtiruvchi issiqlik bilan ishlov berish, donalararo korroziya, don o'lchami, NACE 0175, ikki darajali, payvand chokining parchalanishi, magnit zarrachalarni aniqlash, PWHT (POST PAYVANDA issiqlik bilan ishlov berish), egilish, qattiqlik, Kuchlanish sinovi va boshqalar
Hajmi Barcha naychalar ASTM va ASME kabi tegishli standartlarga muvofiq ishlab chiqariladi va sinovdan o'tkaziladi / tekshiriladi
Qo'shilgan qiymat xizmatlari Chizish / Kengaytirish / Issiqlik bilan ishlov berish / Tavlangan / Ishlov berish / Qumni portlatish / Otishma / Yorqin tavlangan

ASTM A269 standart choksiz quvur kimyoviy tarkibi

ASTM A269 choksiz quvurlar navlari UNS C Mn P S Si Cr Ni Mo
ASTM A269 304 S30400 0.08 2 0.045 0.03 1 18.0-20.0 8.0-11.0  
ASTM A269 304L S30403 0.035 2 0.045 0.03 1 18.0-20.0 8.0-13.0  
ASTM A269 316 S31600 0.08 2 0.045 0.03 1 16.0-18.0 11.0-14.0 2.0-3.0
ASTM A269 316L S31603 0.035 2 0.045 0.03 1 16.0-18.0 10.0-14.0 2.0-3.0

ASTM A269 Elektropolish naychasining mexanik xususiyatlari

Material Issiqlik Harorat Mustahkamlik chegarasi Hosildorlik kuchi Uzayish %, min
Davolash Min. Ksi (MPa), min. Ksi (MPa), min.
  º F(º C)    
ASTM A269 304 Yechim 1900 (1040) 75(515) 30(205) 35
ASTM A269 304L Yechim 1900 (1040) 70(485) 25(170) 35
ASTM A269 316 Yechim 1900(1040) 75(515) 30(205) 35
ASTM A269 316L Yechim 1900(1040) 70(485) 25(170) 35

ASTM A269 zanglamaydigan po'lat quvurlar

astm a269 seamless stainless steel tubinga269 stainless tubing

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

SS quvurlari yetkazib beruvchi-GNEE

GNEE guruhi barcha turdagi qotishma po'lat, zanglamaydigan po'lat, karbonli po'lat, yuqori haroratli, past haroratli va korroziyaga chidamli quvurlar, quvur qismlari va payvandlash materiallari, zanglamaydigan po'lat quvurlar, yuqori nikelli qotishma zanglamaydigan po'lat quvurlarga ixtisoslashgan va Xitoyning eng yaxshi o'nta po'lat yetkazib beruvchilaridan biri. Istalgan vaqtda so'rashingiz mumkin.