JIS G3445 quvur materiali nima

JIS 3445 po'lat quvurlari mashinalar, avtomobillar, velosipedlar, mebellar, jihozlar va boshqa mexanik qismlarga mos keladi. Asosiy navlar: STKM11A, STKM12(A,B,C), STKM12(A,B,C), STKM(A,B,C).

JIS 3445 STKM11, STKM12, STKM13 va STKM14 mexanik quvurlarining kimyoviy tarkibi quyidagi jadvalda keltirilgan:

Baho Kimyoviy tarkibi %
C Si Mn P S Nb yoki V
STKM11A 0 dan kichik yoki unga teng.12 0 dan kichik yoki unga teng.35 0 dan kichik yoki unga teng.60 0 dan kichik yoki unga teng.040 0 dan kichik yoki unga teng.040
STKM12A 0 dan kichik yoki unga teng.20 0 dan kichik yoki unga teng.35 0 dan kichik yoki unga teng.60 0 dan kichik yoki unga teng.040 0 dan kichik yoki unga teng.040 -
STKM12B
STKM12C
STKM13A 0 dan kichik yoki unga teng.25 0 dan kichik yoki unga teng.35 0.30~
0.90
0 dan kichik yoki unga teng.040 0 dan kichik yoki unga teng.040 -
STKM13B
STKM13C
STKM14A 0 dan kichik yoki unga teng.30 0 dan kichik yoki unga teng.35 0.30~
1.00
0 dan kichik yoki unga teng.040 0 dan kichik yoki unga teng.040 -
STKM14B
STKM14C

JIS 3445 STKM11, STKM12, STKM13 va STKM14 karbonli po'latdan yasalgan mexanik quvurlarning mexanik xususiyatlari quyidagi jadvalda keltirilgan:

Baho Mexanik xususiyatlar Yassilash testi Bükme testi
Mustahkamlik chegarasi
(MPa)
Hosildorlik kuchi
(MPa)
Uzayish (%) Masofa
orasida
bu qismlar
(D=OD)
Bukish
Burchak
Ichkarida
Radius
(D=OD)
№ 11: Namuna
STKM11A 230
(294)
- 235 1/2D 180 daraja 4D
STKM12A 235
(343)
218
(177)
235 2/3D 90 daraja 6D
STKM12B 240
(392)
228
(275)
225 2/3D 90 daraja 6D
STKM12C 248
(471)
236
(353)
220 - - -
STKM13A% 3b 238
(373)
222
(216)
230 2/3D 90 daraja 6D
STKM13B 245
(441)
231
(304)
220 3/4D 90 daraja 6D
STKM13C 252
(510)
239
(382)
215 - - -
STKM14A 242
(412)
225
(245)
225 3/4D 90 daraja 6D
STKM14B 251
(500)
236
(353)
215 7/8D 90 daraja 8D
STKM14C 256
(549)
242
(412)
215 - - -

JIS G3445 STKM12A/STKM12B trubkasining tashqi diametrdagi tolerantliklari:

№ 1: tashqi diametri qachon<50mm, tolerance 0.5mm;when outer diameter ≥50 mm,tolerance +/- 0.1mm;

№ 2: tashqi diametri bo'lganda<50mm, tolerance 0.25mm;when outer diameter ≥50 mm,tolerance +/- 0.5mm;

№ 3: tashqi diametri bo'lganda<25mm, tolerance 0.12mm;when 25mm ≤od ≥40 mm,tolerance +/- 0.15mm;

40 mm od dan kichik yoki teng bo'lganda 50 mm dan katta yoki unga teng, bardoshlik +/- 0,18 mm.