A269 payvandlangan ferrit trubkasi
Ferritik po'lat deganda xrom miqdori 14% dan ortiq bo'lgan past uglerodli xromli zanglamaydigan po'lat va xrom miqdori 27% dan ortiq bo'lgan har qanday uglerodli xromli zanglamaydigan po'latdir. Ushbu toifaga tegishli Crl7, Cr17Mo2Ti, Cr25, Cr25Mo3Ti, Cr28 va boshqalar.
So'rov yuborish
Hozir chat
Mahsulotni tanishtirish
Söndürülmüş (qattiq eritma) holatidagi ferrit po'latning tuzilishi ferrit bo'lib, tavlangan va qarigan holatning tuzilishida oz miqdorda karbidlar va intermetalik birikmalarni ko'rish mumkin.
A269 zanglamaydigan po'latdan payvandlangan quvurlarning spetsifikatsiyasi
| Standart | ASTM A268, ASME SA268 |
|---|---|
| Quvur turi | Ham payvandlangan, ham choksiz |
| Baholar | ASTM A268 TP 410, ASTM A268 TP 430, ASTM A268 TP 439 |
| Tashqi diametri | 1/4 dyuym (6,25 mm) dan 8 dyuymgacha (203 mm) |
| Devor qalinligi | {0}}.02" (0,5 mm) dan 0,5" (12 mm) gacha |
| Ilova | Issiqlik almashtirgich, isitgich, kondensator |
ASTM A269 zanglamas po'latdan yasalgan quvurlar o'lchamlari bardoshliligi
| Tashqi diametri, In.[Mm] | OD tolerantligi, In.[Mm] | Devor qalinligi, % | Yupqa devor quvurlari |
|---|---|---|---|
| 1⁄2 gacha, [12,7], tashqari | ±0.005 [0.13] | ±15 | |
| 1⁄2 To 11⁄2 [12.7 To 38.1], Excl/Td> | ±0.005 [0.13] | ±10< | 0,065 dyuymdan kam. [1,6 mm] Nominal |
| 11⁄2 dan 31⁄2 gacha [38,1 dan 88,9 gacha], tashqari | ±0.010 [0.25] | ±10 | 0,095 dyuymdan kam. [2,4 mm] Nominal |
| 31⁄2 dan 51⁄2 gacha [88,9 dan 139,7 gacha], tashqari | ±0.015 [0.38] | ±10 | 0.150 dyuymdan kam. [3,8 mm] Nominal |
| 51⁄2 dan 8 gacha [139,7 dan 203,2 gacha], shu jumladan | ±0.030 [0.76] | ±10 | 0.150 dyuymdan kam. [3,8 mm] Nominal |
ASTM A268 payvandlangan trubaning kuchlanishiga qo'yiladigan talablar
| Baho va UNS belgisi | Kuchlanish kuchi, min, | Hosildorlik kuchi, min, | Cho'zilishA B, 2 dyuymda. Yoki 50 mm, |
|---|---|---|---|
| Ksi % 5bMPa% 5d | Ksi % 5bMPa% 5d | Min% 2c % 25 | |
| TP405 S40500 | 60 [415] | 30 [205] | 20 |
| … S40800 | 55 [380] | 30 [205] | 20 |
| TP410 S41000 | 60 [415] | 30 [205] | 20 |
| TP429, TP430 va TP430 Ti S429000, S 43000 va S 43036 | 60 [415] | 35 [240] | 20 |
| TP443 S44300 | 70 [485] | 40 [275] | 20 |
| TP446-1 S44600 | 70 [485] | 40 [275] | 18 |
| TP446-2 S44600 | 65 [450] | 40 [275] | 20 |
| TP409 S40900 | 55 [380] | 25 [170] | 20 |
| TP439 S43035 | 60 [415] | 30 [205] | 20 |
| S43932 | 60 [415] | 30 [205] | 20 |
| … S41500 | 115 [795] | 90 [620] | 15 |
Kvadrat payvandlangan quvur