ASTM A268 TP410 zanglamaydigan po'lat quvur
Standart martensitik zanglamaydigan po'latlar quyidagilardir: 410, 414, 416, 416 (Se), 420, 431, 440A, 440B va 440C turlari, ular magnitdir; bu po'latlar korroziyaga chidamliligi 11,5 dan 18 foizgacha bo'lgan "xrom" dan kelib chiqadi va xrom miqdori qanchalik yuqori bo'lsa, uglerod miqdori shunchalik yuqori bo'lishini ta'minlash uchun xrom miqdori qanchalik yuqori bo'lsa, uglerod miqdori shunchalik yuqori bo'ladi. issiqlik bilan ishlov berish jarayonida martensit hosil bo'lishini ta'minlash.
A268 payvandlangan zanglamaydigan po'lat quvur spetsifikatsiyasi
|
Standart |
ASTM A268 |
|
Material |
TP405, TP410, TP430, TP446-1, TP446-2, 26-3-3, boshqa materiallar ham mavjud |
| O.D. | 3.2 - 200 mm |
| W.T. | 0.5 - 30 mm |
| Uzunlik | Maksimal 12000 mm |
A268 zanglamaydigan po'latdan payvandlangan quvur kimyoviy tarkibi
|
Baho |
UNS |
C |
Mn |
P |
S |
Ni |
Cr |
Mo |
N |
|
TP410 |
S41000 |
0.15 maks |
1.00 maks |
0.040 maks |
0.030 maks |
--- |
11.5-13.5 |
--- |
--- |
|
|
S42035 |
0.08 maks |
1.00 maks |
0.045 maks |
0.030 maks |
1.0-2.5 |
13.5-15.5 |
--- |
0.30-0.50 |
|
TP430 |
S43000 |
0.12 maks |
1.00 maks |
0.040 maks |
0.030 maks |
--- |
16.0-18.0 |
--- |
--- |
|
TP446-1 |
S44600 |
0.025 maks |
1,50 maksimal |
0.040 maks |
0.030 maks |
0 dan kichik yoki unga teng.75 |
23-27 |
--- |
0.025 maks |
|
TP446-2 |
S44600 |
0.012 maks |
1,50 maksimal |
0.040 maks |
0.030 maks |
0 dan kichik yoki unga teng.50 |
23-27 |
--- |
0.025 maks |
|
26-3-3 |
S44660 |
0.030 maks |
1,50 maksimal |
0.040 maks |
0.030 maks |
1.0-3.5 |
25-28 |
--- |
0.040 maks |
A268 zanglamas po'latdan yasalgan quvur valentlik va qattiqlik talablari
|
Baho |
UNS |
Kuchlanish kuchi, min ksi MPa |
Chidamlilik kuchi, min ksi MPa |
2 dyuym yoki 50 mm cho'zilish, min % |
Rokvell qattiqligining B shkalasi |
|
TP410 |
S41000 |
60 (415) |
30 (205) |
20 |
95 |
|
|
S42035 |
80 (550) |
55 (380) |
16 |
88 |
|
TP430 |
S43000 |
60 (415) |
35 (240) |
20 |
90 |
|
TP446-1 |
S44600 |
70 (485) |
40 (275) |
18 |
95 |
|
TP446-2 |
S44600 |
65 (450) |
40 (275) |
20 |
95 |
|
26-3-3 |
S44660 |
85 (585) |
65 (450) |
20 |
25 |
Martensiti zanglamaydigan po'latdan payvandlangan quvur


Issiq teglar: astm a268 tp410 zanglamaydigan po'lat quvur, Xitoy astm a268 tp410 zanglamaydigan po'lat quvur ishlab chiqaruvchilari, etkazib beruvchilari
Sizga ham yoqishi mumkin
So'rov yuborish